Geri Dön

Florografen katkılı reçine esaslı dental adezivlerin fizikokimyasal ve mekanik özelliklerinin incelenmesi

Investigation of the physicochemical and mechanical properties of fluorographene reinforced resin-based dental adhesives

  1. Tez No: 1026739
  2. Yazar: AYSU SANCAK YÜCETAŞ
  3. Danışmanlar: DOÇ. DR. AYSU AYDINOĞLU
  4. Tez Türü: Yüksek Lisans
  5. Konular: Biyoteknoloji, Diş Hekimliği, Metalurji Mühendisliği, Biotechnology, Dentistry, Metallurgical Engineering
  6. Anahtar Kelimeler: Belirtilmemiş.
  7. Yıl: 2026
  8. Dil: Türkçe
  9. Üniversite: Yıldız Teknik Üniversitesi
  10. Enstitü: Fen Bilimleri Enstitüsü
  11. Ana Bilim Dalı: Biyoteknoloji Ana Bilim Dalı
  12. Bilim Dalı: Biyoteknoloji Bilim Dalı
  13. Sayfa Sayısı: Belirtilmemiş.

Özet

Rezin esaslı dental adeziv sistemlerde su emilimi, hidrolitik degradasyon ve polimer ağ yapısındaki zayıflama, uzun dönem klinik başarıyı sınırlayan önemli faktörlerdir. Bu çalışmada, iki boyutlu grafen türevi bir nanomalzeme olan florografenin deneysel rezin esaslı dental adeziv/reçine formülasyonlarında nano- katkı olarak kullanım potansiyeli araştırılmıştır. Bu amaçla florografen içermeyen kontrol grubu (G0), ağırlıkça %0,1 florografen içeren G1 grubu ve ağırlıkça %0,5 florografen içeren G2 grubu hazırlanmıştır. Hazırlanan formülasyonlar; su emilimi, suda çözünürlük, eğme dayanımı, FTIR ile monomer dönüşüm derecesi, temas açısı, XPS ve FESEM analizleri ile değerlendirilmiştir. Elde edilen bulgular, florografen katkısının deneysel adeziv/reçine matris özelliklerini katkı oranına bağlı olarak değiştirdiğini göstermiştir. Eğme dayanımı sonuçlarında özellikle %0,5 florografen içeren G2 grubunda mekanik dayanımın arttığı belirlenmiştir. Bu durum, florografenin reçine matrisi içerisinde takviye fazı olarak görev yapabileceğini ve iki boyutlu tabakalı yapısı sayesinde gerilme transferine katkı sağlayarak çatlak ilerlemesini sınırlandırabileceğini düşündürmektedir. Böylece florografen katkısının, adeziv tabakanın mekanik yükler altında yapısal xiv bütünlüğünü korumasına katkı sağlayabileceği değerlendirilmiştir. FTIR analizleri, düşük oranlarda florografen ilavesinin monomer dönüşüm derecesini belirgin şekilde olumsuz etkilemediğini göstermiştir. Bu sonuç, florografenin uygun oranlarda kullanıldığında polimerizasyon verimliliğini koruyabilen bir nano-katkı olarak değerlendirilebileceğini ortaya koymaktadır. Temas açısı sonuçlarında ise tüm grupların hidrofilik yüzey karakterini koruduğu belirlenmiş ve florografen katkısının mevcut formülasyonda yüzey hidrofobisitesini belirgin biçimde artırmadığı görülmüştür. XPS analizlerinde florografen içeren gruplarda karbon oranında değişim gözlenmekle birlikte, F1s sinyalinin belirgin olarak saptanmaması florografenin analiz edilen en üst yüzey tabakasında sınırlı düzeyde bulunduğunu veya tespit sınırının altında kaldığını düşündürmektedir. FESEM görüntüleri ise florografen katkısının yüzey morfolojisinde katkı oranına bağlı değişiklikler ve lokal heterojenlikler oluşturabildiğini göstermiştir. Sonuç olarak, florografenin mevcut deneysel dental adeziv/reçine formülasyonunda beklenen hidrofobik yüzey etkisini belirgin biçimde göstermediği, ancak özellikle %0,5 katkı oranında mekanik dayanımı destekleyebilecek potansiyel bir nano-katkı olduğu belirlenmiştir. Florografenin olası avantajının, yüzey hidrofobisitesinden çok mekanik takviye, polimer matris stabilizasyonu ve adeziv tabakanın yapısal bütünlüğünü destekleme yönünde ortaya çıkabileceği değerlendirilmiştir. Bu etkinin dentin-rezin arayüzündeki performansa yansımasının belirlenebilmesi için bağlanma dayanımı, yaşlandırma ve uzun dönem degradasyon çalışmalarına ihtiyaç vardır.

Özet (Çeviri)

Water sorption, hydrolytic degradation, and deterioration of the polymer network are among the major factors limiting the long-term clinical performance of resin- based dental adhesive systems. In this study, the potential use of fluorographene, a two-dimensional graphene derivative nanomaterial, as a nano-reinforcing additive in experimental resin-based dental adhesive formulations was investigated. For this purpose, three experimental groups were prepared: a fluorographene-free control group (G0), a group containing 0.1 wt.% fluorographene (G1), and a group containing 0.5 wt.% fluorographene (G2). The prepared formulations were characterized in terms of water sorption, water solubility, flexural strength, degree of conversion determined by FTIR spectroscopy, contact angle, X-ray photoelectron spectroscopy (XPS), and field emission scanning electron microscopy (FESEM). The results demonstrated that fluorographene incorporation altered the properties of the experimental adhesive/resin matrix depending on the filler concentration. Flexural strength testing revealed an improvement in mechanical performance, particularly in the G2 group containing 0.5 wt.% xvi fluorographene. This finding suggests that fluorographene may act as a reinforcing phase within the resin matrix and contribute to stress transfer through its two- dimensional layered structure, thereby limiting crack propagation. Consequently, fluorographene incorporation may enhance the structural integrity of the adhesive layer under mechanical loading conditions. FTIR analysis indicated that low concentrations of fluorographene did not adversely affect the degree of monomer conversion. This result suggests that fluorographene can be incorporated into adhesive formulations without significantly compromising polymerization efficiency. Contact angle measurements showed that all groups maintained a hydrophilic surface character, indicating that fluorographene incorporation did not result in a pronounced increase in surface hydrophobicity under the conditions investigated. Although XPS analysis revealed changes in surface carbon content, no distinct F1s signal was detected, suggesting that fluorographene was either absent from the outermost analyzed surface layer or present below the detection limit. FESEM observations demonstrated concentration-dependent changes in surface morphology and the presence of localized heterogeneities associated with fluorographene incorporation. In conclusion, although fluorographene did not produce a marked hydrophobic surface effect in the experimental adhesive formulations, it exhibited potential as a nano-reinforcing additive, particularly at a concentration of 0.5 wt.%, by improving mechanical performance. The findings suggest that the primary benefit of fluorographene may be related to mechanical reinforcement, polymer matrix stabilization, and preservation of the structural integrity of the adhesive layer rather than enhancement of surface hydrophobicity. Further studies involving bond strength evaluation, artificial aging, and long-term degradation analyses are required to determine the influence of fluorographene on the dentin–resin interface and clinical performance.

Benzer Tezler

  1. Functionalization of graphene and stoichiometric graphene derivatives

    Grafinin fonksiyonelleştirilmesi ve stokiyometrik grafin türevleri

    HASAN ŞAHİN

    Doktora

    İngilizce

    İngilizce

    2011

    İhsan Doğramacı Bilkent Üniversitesi

    Malzeme Bilimi ve Nanoteknoloji Ana Bilim Dalı (disiplinlerarası)

    Yükleniyor...

  2. Effects of charging on two-dimensional honeycomb nanostructures

    Elektriksel yüklenmenin iki boyutlu bal peteği örgüsüne sahip nanoyapılar üzerine etkisi

    MEHMET TOPSAKAL

    Doktora

    İngilizce

    İngilizce

    2012

    İhsan Doğramacı Bilkent Üniversitesi

    Malzeme Bilimi ve Nanoteknoloji Ana Bilim Dalı (disiplinlerarası)

    Yükleniyor...

  3. Metabolit tayinine yönelik biyoesinlenmiş nanomalzemelerin geliştirilmesi ve uygulamaları

    Development and applications of bioinspired nanomaterials for metabolite detection

    ERDOĞAN ÖZGÜR

    Doktora

    Türkçe

    Türkçe

    2016

    Hacettepe Üniversitesi

    Kimya Ana Bilim Dalı

    Yükleniyor...