Geri Dön

Seçici lazer ergitme yöntemi ile üretilen ınconel 718 numunelerine uygulanan ısıl işleminin işlenebilirlik üzerine etkisinin incelenmesi

Investigation of the effect of heat treatment applied to inconel 718 samples produced by selective laser melting method on machinability

  1. Tez No: 1029368
  2. Yazar: FULYA CEMALOĞLU
  3. Danışmanlar: PROF. DR. HALİL DEMİR, DOÇ. DR. BARIŞ ÖZLÜ
  4. Tez Türü: Doktora
  5. Konular: Makine Mühendisliği, Mechanical Engineering
  6. Anahtar Kelimeler: Belirtilmemiş.
  7. Yıl: 2026
  8. Dil: Türkçe
  9. Üniversite: Karabük Üniversitesi
  10. Enstitü: Lisansüstü Eğitim Enstitüsü
  11. Ana Bilim Dalı: İmalat Mühendisliği Ana Bilim Dalı
  12. Bilim Dalı: Belirtilmemiş.
  13. Sayfa Sayısı: Belirtilmemiş.

Özet

Bu tez çalışmasında, havacılık, uzay ve enerji endüstrilerinde yaygın olarak kullanılan Inconel 718 süper alaşımının farklı üretim yöntemleri ve ısıl işlem koşulları altında mikroyapısal özellikleri, mekanik davranışı ve işlenebilirliği kapsamlı olarak incelenmiştir. Çalışma kapsamında ticari olarak temin edilen dövme numunesi ve Seçici Lazer Ergitme (SLM) yöntemiyle üretilmiş Inconel 718 numuneleri kullanılmıştır. SLM yöntemiyle üretilen numunelere 980 °C'de 1,5 saat çözeltiye alma işlemi uygulanmış, ardından 800 °C'de 1, 4 ve 32 saat sürelerle yaşlandırma işlemleri uygulanmıştır. Üretim yönteminin ve uygulanan ısıl işlemlerin yüzey kalitesi, boyutsal doğruluk, geometrik toleranslar, mikroyapı, sertlik, yoğunluk ve frezeleme performansı üzerindeki etkileri deneysel olarak değerlendirilmiştir. Ayrıca işleme çıktılarının tahmin edilmesi amacıyla yapay zekâ tabanlı makine öğrenmesi modelleri geliştirilmiştir. Deneysel çalışmalar sonucunda, SLM numunelerinin yüzey karakterizasyonu sonucunda ısıl işlemlerin yüzey pürüzlülüğü değerini önemli ölçüde iyileştirdiği belirlenmiştir. Isıl işlem uygulanmamış SLM numunesinde ortalama yüzey pürüzlülük değeri 12,946 µm olarak ölçülürken, en düşük yüzey pürüzlülük değeri 800 °C'de 32 saatlik yaşlandırma sonrasında 10,065 µm olarak elde edilmiş ve yüzey kalitesinde yaklaşık %22,25 oranında iyileşme sağlanmıştır. Buna karşın uzun süreli yaşlandırmanın bazı boyutsal doğruluk ve geometrik tolerans değerlerinde olumsuz değişimlere neden olduğu belirlenmiştir. Mikroyapı incelemeleri sonucunda, SLM numunelerinde dendritik yapı, ergime havuzu izleri ve Laves fazının varlığını ortaya koyarken, çözeltiye alma işlemi sonrasında bu fazların büyük ölçüde çözündüğü ve daha homojen bir mikroyapının oluştuğu tespit edilmiştir. Yaşlandırma işlemleri ile birlikte yapıda γʺ ve γʹ çökeltilerinin oluştuğu, özellikle 800 °C'de 4 saat yaşlandırılan numunenin optimum çökelti dağılımına ulaşarak pik yaşlanma davranışı sergilediği belirlenmiştir. Dövme numunelerde ise homojen ve ince taneli bir yapı gözlenmiştir. Mekanik özellikler bakımından en yüksek sertlik değeri 457 Hv ile dövme numunesinde elde edilirken, SLM-HM numunesinin sertliği ise 303,33 Hv olarak ölçülmüştür. SLM numunesine uygulanan çözeltiye alma işlemi sonrasında sertlik 198 Hv seviyesine düşmüş, ancak yaşlandırma işlemleriyle birlikte yeniden artış göstererek ve en yüksek yaşlandırma sertliğine 800 °C-4 saat koşulunda ulaşılmıştır. Yoğunluk ölçümlerinde dövme numunesi %99,886 bağıl yoğunluk değerine sahipken, SLM-HM numunesinde bu değer %97,912 olarak belirlenmiş, 800 °C'de 4 saatlik yaşlandırma sonrasında ise %98,307 seviyesine yükselmiştir. Frezeleme deneylerinde üretim yöntemi, ısıl işlem koşulları ve soğutma/yağlama stratejilerinin işlenebilirlik üzerinde belirliyeci rolleri olduğu görülmüştür. Deneyler sonucunda kesme kuvveti 276,2 N ile 1185,9 N, yüzey pürüzlülük değeri 0,22 µm ile 1,39 µm ve kesme sıcaklığı 168°C ile 658 °C aralıklarında değişmiştir. En düşük kesme kuvveti 980 °C'de 1,5 saat çözeltiye alma işleminde, en düşük yüzey pürüzlülük değeri ise 800 °C'de 4 saat yaşlandırılmış numunede elde edilmiştir. Takım aşınması bakımından en yüksek aşınma dövme numunesinde gözlemlenirken, ısıl işlem uygulanmış SLM numunelerinde daha düşük takım aşınması meydana gelmiştir. Ayrıca Minimum Miktarda Yağlama (MQL) stratejisinin, kuru işlemeye kıyasla ortalama kesme kuvvetini %15,5, kesme sıcaklığını ise %18,65 oranında azalttığı ve yüzey bütünlüğü ile takım ömrünü iyileştirdiği tespit edilmiştir. İşleme performansının tahmini amacıyla Doğrusal Regresyon (LR), Karar Ağacı Regresyonu (DTR), Destek Vektör Regresyonu (SVR) ve Gauss Süreç Regresyonu (GPR) modelleri geliştirilmiştir. Modeller arasında en yüksek tahmin başarısını gösteren GPR, kesme kuvveti için %98,72, kesme sıcaklığı için ise %98,99 doğruluk oranına ulaşmıştır. Elde edilen bu sonuçlar, makine öğrenmesi yöntemlerinin işleme parametrelerinin optimize edilmesinde güvenilir karar destek araçları olarak kullanılabileceğini ortaya koymaktadır.

Özet (Çeviri)

This thesis comprehensively investigates the microstructural properties, mechanical behavior, and machinability of Inconel 718 superalloy, widely used in the aerospace and energy industries, under different production methods and heat treatment conditions. Commercially available forged specimens and Inconel 718 specimens produced by Selective Laser Melting (SLM) were used in the study. The SLM specimens were subjected to solution treatment at 980 °C for 1.5 hours, followed by aging treatments at 800 °C for 1, 4, and 32 hours. The effects of the production method and applied heat treatments on surface quality, dimensional accuracy, geometric tolerances, microstructure, hardness, density, and milling performance were experimentally evaluated. Furthermore, artificial intelligence-based machine learning models were developed to predict machining outputs. Experimental studies revealed that heat treatments significantly improved the surface roughness of the SLM specimens. In the untreated SLM sample, the average surface roughness value was measured as 12.946 µm, while the lowest surface roughness value of 10.065 µm was obtained after 32 hours of aging at 800 °C, resulting in an improvement in surface quality of approximately 22.25%. However, it was determined that long-term aging caused negative changes in some dimensional accuracy and geometric tolerance values. Microstructure examinations revealed the presence of dendritic structure, melt pool traces, and Laves phase in the SLM samples, while it was found that these phases largely dissolved after solution treatment, resulting in a more homogeneous microstructure. It was determined that γʺ and γʹ precipitates formed in the structure with aging treatments, and that the sample aged at 800 °C for 4 hours reached the optimum precipitate distribution, exhibiting peak aging behavior. In the forged samples, a homogeneous and fine-grained structure was observed. In terms of mechanical properties, the highest hardness value of 457 Hv was obtained in the forged specimen, while the hardness of the SLM-HM specimen was measured as 303.33 Hv. After solution treatment applied to the SLM specimen, the hardness decreased to 198 Hv, but increased again with aging treatments, reaching the highest aging hardness at 800 °C for 4 hours. In density measurements, the forged specimen had a relative density of 99.886%, while this value was determined as 97.912% in the SLM-HM specimen, and increased to 98.307% after aging at 800 °C for 4 hours. In milling experiments, it was observed that the production method, heat treatment conditions, and cooling/lubrication strategies played a decisive role in machinability. Experimental results showed that cutting force ranged from 276.2 N to 1185.9 N, surface roughness from 0.22 µm to 1.39 µm, and cutting temperature from 168°C to 658°C. The lowest cutting force was obtained in the solution treatment at 980°C for 1.5 hours, and the lowest surface roughness was obtained in the sample aged at 800°C for 4 hours. In terms of tool wear, the highest wear was observed in the forged sample, while lower tool wear occurred in the heat-treated SLM samples. Furthermore, it was determined that the Minimum Quantity Lubrication (MQL) strategy reduced the average cutting force by 15.5% and the cutting temperature by 18.65% compared to dry machining, and improved surface integrity and tool life. Linear Regression (LR), Decision Tree Regression (DTR), Support Vector Regression (SVR), and Gaussian Process Regression (GPR) models were developed to predict machining performance. GPR showed the highest prediction accuracy among the models, achieving 98.72% accuracy for cutting force and 98.99% for cutting temperature. These results demonstrate that machine learning methods can be used as reliable decision support tools in optimizing machining parameters.

Benzer Tezler

  1. Seçici lazer ergitme prosesinde Inconel 718 aşınma davranışı

    Wear behaviour of Inconel 718 alloy fabricated by selective laser melting

    BORA ARF

    Yüksek Lisans

    Türkçe

    Türkçe

    2024

    Eskişehir Osmangazi Üniversitesi

    Makine Mühendisliği Ana Bilim Dalı

    Yükleniyor...

  2. SLM yöntemiyle üretilen ınconel 718 numunelerinin talaşlı imalat ve ısıl işlem sonrası yüzey özellikleri ve mikroyapısının incelenmesi

    Inspection of surface properties and microstructure of inconel 718 samples produced by SLM method after machining and heat treatment

    CAN YÜCETEPE

    Yüksek Lisans

    Türkçe

    Türkçe

    2025

    Bursa Uludağ Üniversitesi

    Eklemeli İmalat Ana Bilim Dalı

    Yükleniyor...

  3. Effect of post-processing heat treatment on the mechanical properties of Inconel 718 fabricated by selective laser melting

    İkincil ısıl işlemlerin seçmeli lazer eritme yöntemi ile üretilen Inconel 718 alaşımının mekanik özellikleri üzerindeki etkisi

    SEREN ÖZER

    Yüksek Lisans

    İngilizce

    İngilizce

    2020

    Orta Doğu Teknik Üniversitesi

    Metalurji ve Malzeme Mühendisliği Ana Bilim Dalı

    Yükleniyor...

  4. Inconel 718 süper alaşımının vakum indüksiyon gaz atomizasyon (VIGA) ve lazer toz yataklı ergitme ile prosesi

    Processing of inconel 718 super alloy with vacuum induction gas atomization (VIGA) and laser powder bed fusion

    MÜCTEBA BURAK KARAKAŞ

    Yüksek Lisans

    Türkçe

    Türkçe

    2023

    Bursa Teknik Üniversitesi

    İleri Teknolojiler Ana Bilim Dalı

    Yükleniyor...

  5. Microstructural and mechanical properties of oxide dispersion strengthened inconel 718 alloys produced by selective laser melting

    Seçici lazer ergitme ile üretilen oksit dispersiyonu ile güçlendirilmiş inconel 718 alaşımlarının mikroyapısal ve mekanik özellikleri

    MERVE YEŞİM YALÇIN

    Yüksek Lisans

    İngilizce

    İngilizce

    2023

    Orta Doğu Teknik Üniversitesi

    Metalurji ve Malzeme Mühendisliği Ana Bilim Dalı

    Yükleniyor...