Kaynaklı bağlantılarda kaynak akımının yorulma davranışına etkisinin deneysel ve sayısal karşılaştırılması
Experimental and numerical comparison of the effect of welding current on fatigue behavior in welded joints
- Tez No: 1028202
- Danışmanlar: DOÇ. DR. SEDAT İRİÇ
- Tez Türü: Yüksek Lisans
- Konular: Makine Mühendisliği, Metalurji Mühendisliği, Mechanical Engineering, Metallurgical Engineering
- Anahtar Kelimeler: Deneysel analiz, Mekanik yorulma, Metalografi, Mikroyapı, TIG kaynağı, Experimental analysis, Mechanical fatigue, Metallography, Microstructure, TIG welding
- Yıl: 2025
- Dil: Türkçe
- Üniversite: Sakarya Üniversitesi
- Enstitü: Fen Bilimleri Enstitüsü
- Ana Bilim Dalı: Makine Mühendisliği Ana Bilim Dalı
- Bilim Dalı: Makine Mühendisliği Bilim Dalı
- Sayfa Sayısı: Belirtilmemiş.
Özet
Bu çalışmada, kaynaklı bağlantılarda kaynak parametrelerinin mikro yapı, mekanik özellikler ve yorulma davranışı üzerindeki etkileri deneysel ve sonlu elemanlar analizleri birlikte kullanılarak kapsamlı bir şekilde incelenmiştir. Çalışmanın temel amacı, farklı kaynak akım seviyelerinin yorulma performansı üzerindeki etkisini ortaya koymak ve deneysel sonuçlar ile sayısal analizlerin uyumunu değerlendirmektir. Bu kapsamda, S355J2 yapısal çeliğinden üretilmiş çift T birleşimli numuneler MIG/MAG kaynak yöntemi kullanılarak üç farklı akım seviyesinde (düşük, normal ve yüksek akım) hazırlanmıştır. Bu akım seviyeleri sırasıyla yetersiz, optimum ve aşırı ısı girdisini temsil edecek şekilde seçilmiştir. Kaynak işlemi sonrasında numuneler yorulma testlerine tabi tutulmuş ve kırılmaya kadar geçen çevrim sayıları belirlenmiştir. Deneysel sonuçlara göre, düşük akım numunelerinde ortalama yorulma ömrü 141.956 çevrim, normal akım numunelerinde 201.800 çevrim ve yüksek akım numunelerinde 174.960 çevrim olarak elde edilmiştir. Bu sonuçlar, yorulma ömrünün akım seviyesine doğrusal olarak bağlı olmadığını, belirli bir optimum aralıkta maksimum değere ulaştığını göstermektedir. En yüksek yorulma ömrünün normal akım seviyesinde elde edilmesi, bu parametrenin kaynak kalitesi açısından en uygun koşulları sağladığını ortaya koymaktadır. Kırılma yüzeyi incelemeleri sonucunda, tüm numunelerde çatlak başlangıcının kaynak ayağı bölgesinde gerçekleştiği belirlenmiştir. Düşük akım numunelerinde bağ hataları ve süreksizlikler nedeniyle erken çatlak oluşumu gözlenirken, normal akım numunelerinde daha homojen bir kırılma yüzeyi ve kararlı çatlak ilerleme davranışı tespit edilmiştir. Yüksek akım numunelerinde ise aşırı ısı girdisine bağlı olarak oluşan geniş ITAB ve tane büyümesi, kırılma davranışını olumsuz yönde etkilemiştir. Sertlik ölçümleri incelendiğinde, normal akım numunelerinde daha dengeli ve uygun sertlik dağılımı elde edildiği görülmüştür. Düşük akım numunelerinde sertlik değerlerinin düzensiz dağılımı ve kaynak kusurları, yorulma ömrünün düşmesine neden olurken, yüksek akım numunelerinde ısıl etkiler nedeniyle mekanik özelliklerin zayıfladığı belirlenmiştir. Bu durum, yorulma davranışının yalnızca sertlik değerlerine bağlı olmadığını, aynı zamanda kaynak geometrisi, mikroyapı ve kusur oluşumu gibi faktörlerin birlikte etkili olduğunu göstermektedir. Deneysel çalışmaların yanı sıra, hot spot gerilme yöntemi, effective notch stress yöntemi ve seam weld integrasyon yöntemi kullanılarak sonlu elemanlar analizleri gerçekleştirilmiştir. Elde edilen sonuçlar karşılaştırıldığında, seam weld integrasyon yöntemi ile elde edilen yorulma ömrü değerinin deneysel sonuçlarla yüksek uyum gösterdiği belirlenmiştir. Bu yöntem, kritik düzlem yaklaşımı ile daha gerçekçi sonuçlar sunarken, hot spot yöntemi mühendislik uygulamaları için pratik bir yaklaşım sağlamaktadır. Effective notch stress yöntemi ise daha güvenli tarafta kalan konservatif sonuçlar üretmiştir. Sonuç olarak, kaynak akımının yorulma performansı üzerinde kritik bir parametre olduğu ve optimum akım seviyesinin doğru belirlenmesinin büyük önem taşıdığı ortaya konmuştur. Ayrıca, deneysel veriler ile xxi sayısal analizlerin birlikte değerlendirilmesinin, kaynaklı yapıların yorulma davranışının doğru şekilde anlaşılmasına önemli katkı sağladığı belirlenmiştir. Bu çalışma, hem akademik araştırmalar hem de endüstriyel uygulamalar için yol gösterici nitelikte sonuçlar sunmaktadır.
Özet (Çeviri)
Welded joints are widely used in engineering structures because of their high loadcarrying capacity, manufacturing efficiency, design flexibility, and suitability for industrial applications. They are commonly used in steel structures, automotive components, agricultural machinery, heavy-duty equipment, pressure vessels, and many other structural systems. However, welded joints are also highly sensitive to fatigue damage due to the local effects created by the welding process. During welding, the material is exposed to rapid heating and cooling cycles, which cause microstructural transformations, residual stresses, hardness variations, geometrical discontinuities, and the formation of a heat-affected zone. These effects become especially critical under cyclic loading conditions, where fatigue cracks may initiate and propagate even when the applied stress level is lower than the static strength of the material. The main purpose of this thesis is to investigate the effect of welding current on the fatigue behavior of welded joints by using both experimental methods and finite element-based numerical analyses. In this context, double T-joint specimens were manufactured from S355J2 structural steel using the MIG/MAG welding process. Three different welding current levels were selected as low current, normal current, and high current. These current levels were chosen to represent insufficient heat input, optimum heat input, and excessive heat input conditions, respectively. In this way, the influence of welding current on weld quality, microstructure, hardness distribution, crack initiation behavior, fatigue life, and numerical fatigue predictions was evaluated in a comprehensive manner. S355J2 structural steel was selected as the base material due to its widespread use in welded engineering structures and its suitable mechanical properties for structural applications. The specimens were designed in a double T-joint geometry in order to create a representative welded joint configuration where stress concentration occurs around the weld toe region. After the welding process, the specimens were classified according to their welding current levels. Experimental studies included fatigue tests, macrostructural and microstructural examinations, hardness measurements, fracture surface observations, and strain gauge measurements. Thus, the study was not limited to determining the number of cycles to failure, but also aimed to explain the reasons behind the observed fatigue behavior. Fatigue tests were performed under controlled cyclic loading conditions, and the number of cycles to failure was recorded for each specimen. The experimental results showed that welding current had a significant effect on fatigue life. The average fatigue life of the low current specimens was obtained as 141,956 cycles. The normal current specimens exhibited the highest fatigue performance, with an average fatigue life of 201,800 cycles. The high current specimens showed an average fatigue life of 174,960 cycles. xxiii These results clearly indicate that fatigue life does not increase linearly with increasing welding current. Instead, fatigue performance reaches its maximum value within an optimum welding current range. The normal current specimens showed approximately 36% higher fatigue life than the low current specimens and approximately 15% higher fatigue life than the high current specimens. This result demonstrates that both insufficient and excessive heat input can reduce the fatigue performance of welded joints. In the low current condition, the heat input was not sufficient to provide ideal weld formation and penetration. This may lead to welding defects such as lack of fusion, discontinuities, and irregular weld geometry. These defects act as stress concentration points and accelerate fatigue crack initiation. In the high current condition, although penetration may increase, excessive heat input causes a wider heataffected zone, grain coarsening, and microstructural heterogeneity. These changes negatively affect the fatigue resistance of the welded joint. Fracture surface examinations showed that fatigue cracks initiated mainly from the weld toe region in all specimen groups. This result is consistent with the general fatigue behavior of welded joints, since the weld toe is one of the most critical regions due to geometrical discontinuity and local stress concentration. In the low current specimens, irregular fracture surfaces and early crack initiation were observed due to insufficient weld quality and possible welding defects. In the normal current specimens, the fracture surfaces were more uniform, and crack propagation was more stable. This indicates that the normal current condition provided better weld quality and a more homogeneous structure. In the high current specimens, the fracture behavior was affected by excessive heat input, a wider heat-affected zone, and microstructural coarsening. Hardness measurements were performed across the weld metal, heat-affected zone, and base material to evaluate the mechanical property distribution in the welded joint. The results showed that hardness values alone are not sufficient to explain fatigue behavior. Although hardness distribution is an important indicator of local mechanical properties, fatigue performance is also strongly affected by weld geometry, defect formation, microstructural homogeneity, heat-affected zone width, and local stress concentration. The normal current specimens exhibited a more balanced hardness distribution compared to the low and high current specimens. This balanced distribution contributed to the higher fatigue life obtained under the normal current condition. In addition to the experimental investigations, finite element analyses were performed to predict the fatigue behavior of the welded joints. Three different fatigue assessment methods were used: the structural hot spot stress method, the effective notch stress method, and the seam weld integration method. The finite element model was prepared by considering the specimen geometry, boundary conditions, loading conditions, and weld region representation. The numerical results were compared with the experimental fatigue test results in order to evaluate the accuracy and applicability of these methods. The structural hot spot stress method provided a practical engineering approach for evaluating fatigue behavior in welded joints. This method is useful because it focuses on the structural stress at critical weld regions. However, since it does not fully represent the local notch effect at the weld toe, some deviation from the experimental results may occur. The effective notch stress method, on the other hand, considers local stress concentration more explicitly by using a reference notch radius. Therefore, it produced more conservative fatigue life predictions. xxiv This conservative behavior can be useful for safe design, especially when local weld geometry and notch effects are critical. Among the numerical methods used in this study, the seam weld integration method showed the best agreement with the experimental results. The fatigue life predicted by this method was approximately 201,900 cycles, which is very close to the average experimental fatigue life of the normal current specimens. This agreement indicates that the seam weld integration method can successfully represent the fatigue behavior of welded joints under optimum welding conditions. It also shows that advanced finite element-based fatigue methods can be effective tools for fatigue life prediction when the weld geometry, material properties, boundary conditions, and loading conditions are properly defined. As a general conclusion, welding current is a critical parameter that directly affects the fatigue performance of welded joints. Low welding current may cause insufficient fusion, discontinuities, and early crack initiation, while high welding current may lead to excessive heat input, wider heat-affected zones, grain coarsening, and unfavorable microstructural changes. The best fatigue performance was obtained under the normal current condition, which provided a balanced weld structure, more stable crack propagation behavior, and higher fatigue resistance. This thesis shows that fatigue behavior in welded joints is controlled by a combination of welding parameters, weld geometry, microstructure, hardness distribution, defect formation, and local stress concentration. Therefore, experimental results and numerical analyses should be evaluated together for a reliable understanding of welded joint fatigue behavior. The findings of this study provide useful guidance for the selection of welding parameters, the improvement of fatigue performance, and the numerical fatigue assessment of welded structural components.
Benzer Tezler
- Assessment of operational transfer path analysis for practical applications
Pratik uygulamalar için operasyonel iletim yolu analizi'nin değerlendirilmesi
GÜRKAN TUTU
Yüksek Lisans
İngilizce
2015
İstanbul Teknik ÜniversitesiMakine Mühendisliği Ana Bilim Dalı
Yükleniyor...
- Pamuk ipliklerinde istatiksel bir hata analiz yönteminin geliştirilmesi üzerinde araştırmalar
Başlık çevirisi yok
AYŞE KARAKOR
- Karma yemin fosfor kaynağı ve düzeyinin etlik piliç performansına etkileri üzerinde bir araştırma
Başlık çevirisi yok
SEZEN ÖZKAN SERTER
- Türkiye'de karma yemlerde uygulanan sübvansiyonun çeşitli etkilerinin değerlendirilmesi üzerine bir araştırma
Başlık çevirisi yok
BUKET KARATURHAN