Sonlu elemanlar yöntemi kullanılarak otomotiv titreşim sönümleyici elemanlarında vulkanizasyon derecesinin belirlenmesi ve optimizasyonu
Determination and optimization of the vulcanization degree of automotive vibration damping components using the finite element method
- Tez No: 1032224
- Danışmanlar: DOÇ. DR. MERAL AKKOYUN KURTLU
- Tez Türü: Yüksek Lisans
- Konular: Mühendislik Bilimleri, Engineering Sciences
- Anahtar Kelimeler: Doğal kauçuk, Elastomerler, Enjeksiyon kalıplama, Simülasyon, Sonlu elemanlar yöntemi, Vulkanizasyon, Natural rubber, Elastomers, Injection molding, Finite element method, Vulcanization
- Yıl: 2026
- Dil: Türkçe
- Üniversite: Bursa Teknik Üniversitesi
- Enstitü: Lisansüstü Eğitim Enstitüsü
- Ana Bilim Dalı: Polimer Malzeme Mühendisliği Ana Bilim Dalı
- Bilim Dalı: Polimer Malzeme Mühendisliği Bilim Dalı
- Sayfa Sayısı: Belirtilmemiş.
Özet
Otomotiv titreşim sönümleyici elemanları, motor ve şasi sistemlerinden kaynaklanan titreşimlerin araç gövdesine iletimini azaltan kritik elastomerik bileşenlerdir. Bu parçaların performansı yalnızca kullanılan kauçuk reçetesine değil, üretim sırasında oluşan çapraz bağ ağına, kür derecesine ve bu kürlenmenin parça hacmi boyunca ne kadar homojen gerçekleştiğine bağlıdır. Bu tez çalışmasında, doğal kauçuk esaslı bir otomotiv motor takozunda vulkanizasyon süresinin kür derecesi dağılımı, mekanik davranış, dinamik performans, kalıcı deformasyon, çapraz bağ yoğunluğu, termal kararlılık, kimyasal yapı ve morfolojik bütünlük üzerindeki etkileri incelenmiştir. Çalışma kapsamında doğal kauçuk esaslı motor takozu numuneleri 150 °C kalıp sıcaklığında 6, 8 ve 10 dakikalık vulkanizasyon sürelerinde üretilmiştir. Aynı proses koşulları için SIGMASOFT v6,1 yazılımı kullanılarak sonlu elemanlar yöntemi tabanlı proses simülasyonları gerçekleştirilmiş ve parça hacmi boyunca gelişen kür derecesi dağılımları belirlenmiştir. Malzemenin kür davranışı DSC ve MDR verileri kullanılarak tanımlanmış; sayısal sonuçlar Shore A sertlik ölçümü, statik yük testi, dinamik yük testi, kalıcı deformasyon testi, Flory-Rehner şişme testi, TGA, FT-IR ve SEM analizleriyle deneysel olarak değerlendirilmiştir. Simülasyon sonuçları, 6 dakikalık vulkanizasyon süresinde parça merkezinde kür gelişiminin yetersiz kaldığını ve belirgin bir merkez-çevre kür gradyenti oluştuğunu göstermiştir. Kondisyon sonrasında 8 dakikalık numunede kür derecesi yaklaşık %85–%87 aralığında daha homojen dağılmış, 10 dakikalık numunede ise daha yüksek kür derecelerine ulaşılmıştır. Ancak deneysel bulgular, optimum proses koşulunun yalnızca en yüksek kür derecesi veya en yüksek çapraz bağ yoğunluğu ile belirlenemeyeceğini ortaya koymuştur. Shore A sertlik değeri NR-8 numunede 53,8 olarak belirlenmiş ve ±5 mm deplasman altında en yüksek statik kuvvet 1,352 kN ile yine NR-8 numunede elde edilmiştir. Dinamik testlerde her iki frekansta da en düşük tan δ değerleri NR-8 numunede ölçülmüş, kalıcı deformasyon testinde de en düşük değer %5,8 ile bu numunede bulunmuştur. Flory-Rehner sonuçları çapraz bağ yoğunluğunun vulkanizasyon süresiyle arttığını göstermiş, ancak NR-10 numunenin daha yüksek ağ yoğunluğuna rağmen genel servis performansı bakımından NR-8 numuneyi aşamadığı belirlenmiştir. TGA sonuçları tüm numunelerin doğal kauçuk esaslı yapıya özgü çok aşamalı bozunma davranışı sergilediğini göstermiştir. FT-IR analizlerinde ana kimyasal yapının korunduğu, SEM incelemelerinde ise NR-8 numunenin daha homojen ve daha süreklilik gösteren bir morfolojiye sahip olduğu görülmüştür. Sonuç olarak, incelenen reçete ve geometri için 150 °C'de 8 dakikalık vulkanizasyon süresi optimum proses koşulu olarak belirlenmiştir. Bu çalışma, elastomer esaslı titreşim sönümleyici parçaların üretiminde sonlu elemanlar yöntemi tabanlı proses simülasyonu ile deneysel karakterizasyonun birlikte kullanılmasının, vulkanizasyon süresinin optimize edilmesi ve ürün performansının güvenilir biçimde değerlendirilmesi açısından etkili bir mühendislik yaklaşımı sunduğunu göstermektedir.
Özet (Çeviri)
Automotive vibration damping components are critical elastomeric parts used to reduce the transmission of vibrations generated by the engine and chassis systems to the vehicle body. The performance of these components depends not only on the rubber formulation but also on the crosslinking network formed during production, the degree of cure, and the homogeneity of curing throughout the part volume. In this thesis, the effects of vulcanization time on the cure degree distribution, mechanical behavior, dynamic performance, compression set, crosslink density, thermal stability, chemical structure, and morphological integrity of a natural rubber-based automotive engine mount were investigated. Natural rubber-based engine mount samples were produced at a mold temperature of 150 °C using vulcanization times of 6, 8, and 10 min. For the same process conditions, finite element method-based process simulations were performed using SIGMASOFT v6.1, and the cure degree distributions throughout the component volume were determined. The curing behavior of the material was defined using DSC and MDR data. The numerical results were experimentally evaluated by Shore A hardness measurement, static load testing, dynamic load testing, compression set testing, Flory-Rehner swelling analysis, TGA, FT-IR, and SEM analyses. The simulation results showed that the 6 min vulcanization condition resulted in insufficient cure development in the central region of the part and caused a significant center-to-surface cure gradient. After conditioning, the 8 min sample exhibited a more homogeneous cure degree distribution of approximately 85–87%, while the 10 min sample reached higher cure levels. However, the experimental results demonstrated that the optimum process condition cannot be determined only by the highest cure degree or the highest crosslink density. The Shore A hardness of the NR-8 sample was determined as 53.8, and the highest static force under ±5 mm displacement was also obtained for the NR-8 sample as 1.352 kN. In the dynamic tests, the lowest tan δ values at both evaluated frequencies were measured for the NR-8 sample, indicating a more balanced relationship between stiffness, damping, and elastic recovery. The compression set test also supported this result, with the lowest value of 5.8% obtained for the NR-8 sample. The Flory-Rehner results showed that crosslink density increased with vulcanization time; however, although the NR-10 sample had a higher network density, it did not surpass the overall service performance of the NR-8 sample. TGA results indicated that all samples exhibited a multi-stage thermal degradation behavior characteristic of natural rubber-based elastomeric systems. FT-IR spectra showed that the main chemical structure of the rubber formulation was preserved in all samples. SEM observations revealed that the NR-8 sample had a more homogeneous and continuous morphology, whereas the NR-6 sample showed more pronounced voids and surface discontinuities. As a result, for the investigated formulation and geometry, the vulcanization condition of 8 min at 150 °C was determined as the optimum process condition. This study demonstrates that the combined use of finite element method-based process simulation and experimental characterization provides an effective engineering approach for optimizing vulcanization time and reliably evaluating the performance of elastomeric automotive vibration damping components.
Benzer Tezler
- Nükleer rezonasta moleküler yapıların incelenmesi (yapısal faz geçiş kuramları üzerine bir inceleme)
Başlık çevirisi yok
ABDURRAHMAN ANDİÇ
- İki katlı pamuk ipliklerinden dokunan kumaşlarda örgüye bağlı olarak maksimum atkı sıklığının değişimi üzerinde bir araştırma
Başlık çevirisi yok
MELTEM ASLI NARTER
- Ege bölgesi keçi liflerinin bazı önemli fiziksel, kimyasal özellikleri ve değerlendirme imkanları
Başlık çevirisi yok
NİLÜFER ERDEM