Geri Dön

Dental köprü üretimlerinde, farklı opak malzemelerinin fırınlama sonrası oluşan gerilmeler üzerindeki etkileri

Influences of different opaque materials on stress occured after firing process at dental bridge production

  1. Tez No: 243821
  2. Yazar: DERYA SAATÇI
  3. Danışmanlar: PROF. DR. MEHMET ZOR
  4. Tez Türü: Yüksek Lisans
  5. Konular: Makine Mühendisliği, Mechanical Engineering
  6. Anahtar Kelimeler: Dental porselen, Dental restorasyon, Dental stres analizi, Kalıntı gerilmeleri, Termal gerilme, Dental porcelain, Dental restoration, Dental stress analysis, Residual stresses, Thermal stress
  7. Yıl: 2009
  8. Dil: Türkçe
  9. Üniversite: Dokuz Eylül Üniversitesi
  10. Enstitü: Fen Bilimleri Enstitüsü
  11. Ana Bilim Dalı: Makine Mühendisliği Bölümü
  12. Bilim Dalı: Mekanik Ana Bilim Dalı
  13. Sayfa Sayısı: Belirtilmemiş.

Özet

Bu çalışmada, dental köprü uygulamalarında metal altyapı ve porselen üst yapı arasında bağlayıcı eleman olarak kullanılan farklı opak malzemelerinin, fırınlama sonrası oluşan ısıl gerilmeler üzerindeki etkileri araştırılmıştır.Çalışmada öncelikle dental laboratuarda dört üyeli, CoCr alt destek yapısına sahip köprü hazırlanmıştır. Hazırlanan bu köprü okulumuz bünyesindeki mekanik laboratuarında bulunan özel dental fırında 9600C sıcaklığına kadar standart fırınlama işlemine tabi tutulmuş, fırının kapağı kademeli bir şekilde açılarak ortam sıcaklığına soğuma gerçekleştirilmiştir. Dental köprünün üzerine çeşitli noktalardan bağlanan termokupllar ile bu noktaların sıcaklıkları çeşitli zaman aralıklarında kaydedilerek, soğuma eğrileri çıkarılmıştır. Bu soğuma eğrileri yardımı ile eşdeğer ısı transfer katsayıları sıcaklığa bağlı olarak hesaplanmıştır.Daha sonra SolidWorks programı ile bu dört üyenin modeli kurulmuş ve model ABAQUS programına aktarılarak analizleri yapılmıştır. Hesaplanan ısı transfer katsayıları, sonlu elemanlar programına girilerek soğuma eğrileri numerik olarak da elde edilmiştir. Deneysel olarak elde edilmiş olan soğuma eğrileri ile sonlu elemanlar programı ile elde edilen eğrilerinin yeterli seviyede birbirlerine yakın oldukları gözlenmiştir. Isıl genleşme katsayıları açısından farklılık gösteren 6 tip opak malzeme aynı modelde tanımlanarak, soğuma sırasında ve sonundaki ısıl gerilmeler birbirleriyle karşılaştırılmıştır. Bu şekilde opak malzemelerin birbirlerine göre üstünlükleri tespit edilmeye çalışılmıştır.

Özet (Çeviri)

In this study it was purposed that to examine the thermal stresses occured after firing process at dental bridge applications in changes of opaque material which is used as binding material between metal substructure and porcelain superstructure.First of all a four unit bridge model has been prepared by a dental laboratory. After that this model has been fired up to 9600C at a special oven which exist at our university?s mechanical department?s laboratory. At the end of this process, the oven?s door was opened in stages to get the model?s temperature to ambient temperature. With thermocouples connected to various points on dental bridge, temperatures of these points were saved in various times and we took out the cooling curves. With the help of these cooling curves, we calculated the equivalent heat transfer coefficient according to temperatures.Afterward this four unit?s model was built with SolidWorks and this model was imported to ABAQUS then made the analysis . The cooling curves were obtained numericaly by entering the calculated heat transfer coefficients to finite element analysis program. It has been seen that the cooling curves, we got from experimentally and we got from finite element analysis program, came close in enough ratios. Six kinds of opaque materials which shows diversity interms of thermal expansion coefficients were defined in the same model and thermal stresses which occured during cooling and at the end of cooling were compared. With this, we endeavored to fasten down the advantages of opaque materials to each others.

Benzer Tezler

  1. Co-Cr ve Ni-Cr esaslı kron köprü protezlerin üretimi sürecinde meydana gelebilecek işçi kaynaklı hataların sitotoksik ve genotoksik etkilerinin in vitro koşullarda araştırılması

    In vitro investigation of the cytotoxic and genotoxic effects of the man made errors during the manufacturing process of Co-Cr and Ni-Cr base dental crowns and bridges

    EMRAH ALTAŞ

    Yüksek Lisans

    Türkçe

    Türkçe

    2009

    BiyomühendislikEge Üniversitesi

    Biyomühendislik Ana Bilim Dalı

    PROF. DR. İSMET DELİLOĞLU GÜRHAN

    YRD. DOÇ. AYLİN ŞENDEMİR ÜRKMEZ

  2. Diş destekli üç üyeli ve dört üyeli köprü restorasyonlarında, metal üzerine preslenmiş porselen (POM) ile zirkonyum destekli ve konvansiyonel metal seramik restorasyonların, venerleme öncesi ve sonrası marjinal uyum ve iç uyumlarının karşılaştırılması

    In vitro comparison of marginal and internal fit of press-on-metal ceramic (POM) restorations with zirconium supported and conventional metal ceramic fixed partial dentures before and after veneering

    SEDA VAROL

    Doktora

    Türkçe

    Türkçe

    2014

    Diş HekimliğiMarmara Üniversitesi

    Protetik Diş Tedavisi Ana Bilim Dalı

    PROF. DR. YASEMİN KULAK ÖZKAN

  3. Sabit protetik restorasyonların söküm nedenlerinin ve ağızda kalma sürelerinin değerlendirilmesi

    Evaluation of the reasons for removal of fixed prosthetic restorations and their durations of stay in the mouth

    ZEYNEP CEYLAN

    Diş Hekimliği Uzmanlık

    Türkçe

    Türkçe

    2024

    Diş HekimliğiZonguldak Bülent Ecevit Üniversitesi

    Protetik Diş Tedavisi Ana Bilim Dalı

    DR. ÖĞR. ÜYESİ ŞÜKRİYE ECE GEDUK

  4. İnley destekli ve geleneksel köprülerin kök ve kron yüzeylerinde oluşturdukları stres: Sonlu eleman analizi

    Stress on root and crown surfaces of inlay-supported and conventional bridges: Finite element analysis

    TURHAN ULUTEKİN

    Doktora

    Türkçe

    Türkçe

    2023

    Diş HekimliğiBaşkent Üniversitesi

    Protetik Diş Tedavisi Ana Bilim Dalı

    DOÇ. DR. ÖZLEM ORMAN