Geri Dön

Farklı yüzey hazırlama ve silanlama tekniklerinin CAD-CAM materyallerinin bağlanma dayanımına etkisi

The effect of different surface preparation and silane techniques on the bond strength of CAD-CAM materials

  1. Tez No: 462730
  2. Yazar: MUSTAFA ÇAKIR
  3. Danışmanlar: DOÇ. DR. BİLAL YAŞA, YRD. DOÇ. DR. SERDAR BAĞLAR
  4. Tez Türü: Doktora
  5. Konular: Diş Hekimliği, Dentistry
  6. Anahtar Kelimeler: Belirtilmemiş.
  7. Yıl: 2017
  8. Dil: Türkçe
  9. Üniversite: İzmir Katip Çelebi Üniversitesi
  10. Enstitü: Sağlık Bilimleri Enstitüsü
  11. Ana Bilim Dalı: Restoratif Diş Tedavisi Ana Bilim Dalı
  12. Bilim Dalı: Belirtilmemiş.
  13. Sayfa Sayısı: 137

Özet

Günümüzde CAD-CAM sistemleri ile yapılan restorasyonlar diş hekimliğinde giderek yaygınlaşmaktadır. Bu restorasyonların diş dokularına bağlanmasını sağlayan adeziv sistemlerde de gelişmeler yaşanmaktadır. Yapıştırma simanlarının restorasyona olan bağlanma dayanımı, restorasyonun başarısı açısından önemlidir. Simantasyondan önce materyale uygulanan yüzey hazırlama işlemleri iyi bir adezyon açısından krtik öneme sahiptir. Bu çalışmanın amacı farklı yüzey hazırlama teknikleri ve silanlama prosedürlerinin RelyX Ultimate simanın CAD-CAM materyallerine olan bağlanma dayanımına etkisini değerlendirmektir. Çalışmada Lava Ultimate ve IPS e.max CAD materyalleri kullanılarak oluşturulan parçalara yüzey hazırlama metodu olarak; Cojet, kumlama, HF asit ve Er:YAG lazer uygulandı. Ayrıca hiçbir ajanın uygulanmadığı kontrol grubu elde edildi. Bu grupların kendi içlerinde, silan+adeziv, yalnızca adeziv ve yalnızca silan uygulanan alt grupları elde edildi. Parçalar, RelyX Ultimate ile birbirlerine yapıştırılıp hassas kesme cihazı ile 1mm²'lik test çubukları elde edildi. Örnekler çekme testine tabi tutulup mikrogerilim bağlantı değerleri hesaplandı. Kopma yüzeyleri stereomikroskop ve SEM ile değerlendirildi. Elde edilen değerler ANOVA ve Tukey's HSD testleri ile analiz edildi. Çalışma sonucunda Lava Ultimate'in, IPS e.max CAD'e göre daha yüksek bağlanma değerlerine sahip olduğu gözlendi. Lava Ultimate gruplarında Cojet ve kumlama işlemi diğer yöntemlere göre daha etkili bulundu. IPS e.max CAD gruplarında Cojet işlemi en etkili yöntemken ardından gelen kumlama ve HF asit işlemi arasında anlamlı fark bulunmadı. Er:YAG lazer ise bağlanmayı anlamlı derecede düşürdü. Her iki materyalde de en iyi sonuçlar sırasıyla silan+adeziv, yalnızca adeziv ve yalnızca silan uygulamalarıyla elde edildi.

Özet (Çeviri)

Nowadays, restorations which made using CAD-CAM sytems, are becoming widespread. Also improvements have occured about adhesive systems which enables connection between restoration and tooth structure. Bond strength of luting cements to restorations is important for the success of restorations. Surface treatments applied to material prior to cementation has a critical importance for good adhesion. The aim of this study is to investigate the effects of different surface treatments and silane techniques on bond strenght between RelyX Ultimate cement and CAD-CAM materials. Cojet, sandblasting, HF acid and Er:YAG laser applied as surface treatment method to pieces derived from Lava Ultimate and IPS e.max CAD. In addition, a control group was created. In these groups, silane+adhesive and only adhesive and only silane subgroups was created. The pieces were luted to each other with cement and 1mm2 bars were obtained using precision cutting device. The samples were tested and microtensile bond strength values were calculated. The failure types were evaulated according to stereomicroscope and SEM images. For statistical analyses, ANOVA and Tukey's HSD tests were used. In the conclusion, Lava Ultimate's bond strengt values were higher than, IPS e.max CAD's values. In Lava Ultimate groups, Cojet and sandblasting procedures were more effective than other methods. In IPS e.max CAD groups while Cojet procedure was the most effective, there was no significant difference between ensuing sandblasting and HF acid procedures. Er:YAG laser reduced the bond strength significantly. For both materials, the best results were obtained with silane+adhesive, only adhesive and only silane application respectively.

Benzer Tezler

  1. Numerical model of flue gas desulfurization spray tower in power plant

    Enerji santrallerinde baca gazı kükürt arıtma sistemlerinin nümerik modeli

    OSMAN GÖZÜTOK

    Yüksek Lisans

    İngilizce

    İngilizce

    2018

    Kimyaİstanbul Teknik Üniversitesi

    Uçak ve Uzay Mühendisliği Ana Bilim Dalı

    DR. BAYRAM ÇELİK

  2. Use of sol-gel beads in precon lentration

    Başlık çevirisi yok

    TİJEN EROĞLU

    Yüksek Lisans

    İngilizce

    İngilizce

    1999

    KimyaOrta Doğu Teknik Üniversitesi

    Kimya Ana Bilim Dalı

    DOÇ. DR. MÜRVET VOLKAN

  3. Decision-making mechanism in appropriate roof selection for rainwater harvesting based on combining field data and laboratory experiments

    Yağmur suyu hasadi için uygun çati seçiminde saha verileri ve laboratuvar deneylerine dayali karar verme mekanizmasinin kullanilmasi

    SHAYAN SHITREH

    Yüksek Lisans

    İngilizce

    İngilizce

    2024

    Çevre Mühendisliğiİstanbul Teknik Üniversitesi

    Çevre Mühendisliği Ana Bilim Dalı

    DOÇ. DR. HALE ÖZGÜN ERŞAHİN

  4. Preparation and characterization of anti bacterial, anti scratch and easy to clean multifunctional coatings by sol gel method

    Anti bakteriyel, çizilme direnci yüksek ve kolay temizlenebilen kaplamaların sol jel yöntemiyle hazırlanması ve karakterizasyonu

    FATMA BEYZA YEDİKARDEŞ

    Yüksek Lisans

    İngilizce

    İngilizce

    2016

    Kimyaİstanbul Teknik Üniversitesi

    Nanobilim ve Nanomühendislik Ana Bilim Dalı

    PROF. DR. ESRA ÖZKAN ZAYİM

  5. Application d'entrepot de donnee dans le domaine de gestion de systeme information

    Yönetim bilişim sistemi kapsamında veri ambarı uygulaması

    AKIN MUSTAFA HAPÇIOĞLU

    Yüksek Lisans

    Fransızca

    Fransızca

    2002

    Endüstri ve Endüstri MühendisliğiGalatasaray Üniversitesi

    PROF. DR. ETHEM TOLGA