Geri Dön

Plastik atıkların katalitik ortamda ısı bozunması

Thermal degredation of the waste plastics in catalytic media

  1. Tez No: 47781
  2. Yazar: RAGIP UFUK FIRAT
  3. Danışmanlar: Y.DOÇ.DR. AKİF ŞENER
  4. Tez Türü: Yüksek Lisans
  5. Konular: Kimya Mühendisliği, Chemical Engineering
  6. Anahtar Kelimeler: Belirtilmemiş.
  7. Yıl: 1996
  8. Dil: Türkçe
  9. Üniversite: Ankara Üniversitesi
  10. Enstitü: Fen Bilimleri Enstitüsü
  11. Ana Bilim Dalı: Kimya Mühendisliği Ana Bilim Dalı
  12. Bilim Dalı: Belirtilmemiş.
  13. Sayfa Sayısı: 159

Özet

Bu çalışmada, ceketten elektrikle ısıtılan bir otoklavda endüstriyel Yüksek Yoğunluklu Polietilen (YYPE) atıklarının, n-pentan çözücü ortamında ısıl parçalanma ürünleri incelenmiş; uygun sıcaklık, reaksiyon süresi, besleme oranı, basınç ve katalizör (S1O2) oranı saptanmıştır. YYPE/n-pentan'ın 1:5 besleme oranı ile 360-440°C sıcaklıkları arasında gerçekleştirilen ön denemelerde; 400°C'nin üzerinde, YYPE'nin tamamının parçalanarak gaz ve sıvı ürünlere dönüştüğü ve 405 "C'de sıvı ürün veriminin en yüksek olduğu (% 85,3) bulunmuştur. Reaksiyon süresi 0,5-2 saat arasında değiştirildiğinde; en yüksek sıvı ürün dönüşümü, 1 saatlik reaksiyon süresi sonunda elde edilmiştir. 0,5 saatlik reaksiyon süresinde YYPE'nin tamamen parçalanmadığı; 2 saatlik reaksiyon süresinde de, YYPE'nin tamamının parçalandığı, buna karşlık gaz ürün dönüşümünün arttığı gözlenmiştir. Çözücü oranının artmasının sıvı ürün verimine etkisi araştırılmış ve çözücü miktarının artması ile sıvı ürün veriminin çok az arttığı görülmüştür.Bu artışın az olması ve en az çözücü ile çalışmanın ileride yapılacak araştırmanın, devamına getireceği avantaj gözönüne alınarak 1:1 YYPE/n-pentan oranı, sıvı ürün dönüşüm için uygun bulunmuştur. Bu besleme oranında sıvı ürün verimi % 82,3 olarak elde edilmiştir. 405°C'de 1:1 YYPE/n-pentan oranında otoklava beslenen madde miktarları arttırılarak basıncın artması sağlanmış ve ayarlanan sıcaklığa ulaşıldığı andaki basınç olan 20-42,5 at arasında yapılan denemelerde basıncın, sıvı ürün verimine bir etkisinin olmadığı görülmüştür. % 10 katalizör konularak yapılan denemelerde; aynı şartlarda katalizör konulmadan yapılan deneylere kıyasla sıvı veriminin düştüğü, gaz veriminin arttığı tespit edilmiştir. Deneylerden elde edilen sıvr ürünler, otomatik distilasyon cihazı ite fraksiyonlarına ayrılmış ve 220°C'ye kadar destile edilebilenlerin bileşimindeki alkan, alken, siklik ve aromatik maddelerin; sıcaklık, reaksiyon süresi, besleme oranı ve katalizör ile değişimleri, yapılan GC-MS analizleri ile araştırılmıştır. Gaz ürünlerin ise GC analizleri yapılmış; aynı parametreler ile gaz ürünlerin değişimi incelenmiştir. ANAHTAR KELİMELER : YYPE; Atık Plastik, Isı ite Parçalanma, Gerikazanım, GC-MS Analizleri

Özet (Çeviri)

In this research; Samples of Industrial“High Density Polyethylene (HOPE)”wastes were thermally degredated in a n-pentane medium in an autoklave, investigating the Optimum feed ratio, reaction time, temperature, pressure and catalyst ratio. Preliminary experiments carried out by employing with 1:5 ratio of an HDPE/ n- penlane at 360-440°C showed that HDPE has completely decomposed above 400 °C and the highest liquid yield was obtained approximately at 405 °C as % 83. Reaction time was changed between 0.5-2 hours. The highest liquid coverslon and complete degredation appeared in the first 1 hour. When the temperature was increased, the liquid yield has decreased but gas yield has increased. The effect of the feed ratio was also indicated by changing the ratio of HDPE/n-pentan between 1:0-1 :5.The results showed tiiat addition of more solvent hasn't effected the liquid yield and caused slightly increasing of overall conversion. As a result of experiments and keeping the advantages of using less solvent, 1:1 HDPE/n-pentane ratio was based as a suitable ratio and in this case, the liquid product conversion was found as % 82.3. Investigating the effect of pressure on liquid product conversion; total feed amount was changed as 60, 80 and 100 g by keeping constant of HDPE/n-pentane (1:1).Pressure increased from 20 at. to 42,5 at which are pressure at the point that has been set as temperature. According to catalystless experiments; Using Si02 catalyst has decreased the liquid product and increased the gaseous components. Liquid products obtained from industrial HDPE were fractioned with an automatic distillation apparatus. The fractions distilated below 220 °C were anayzed by GC-MS to determine the effect of feed ratio, reaction time, temperature, pressure and catalyst ratio on the organic groups. The gaseous products were analyzed with GC apparatus and It was only found methane as gaseous product In this case too, It was investigated the effect of feed ratio, reaction time, temperature, pressure and catalyst ratio on the yields of the gaseous products. KEY WORDS: HDPE, Waste Plastics, Degredation, Recycle, GC-MS Analysis.

Benzer Tezler

  1. Metal yüklü zeolit katalizörlerle plastik atıkların kimyasal geri kazanımı

    Chemical recycling of plastic wastes over metal doped zeolite catalysts

    TUĞBA ALBAYRAK

    Yüksek Lisans

    Türkçe

    Türkçe

    2019

    Kimya MühendisliğiAnkara Üniversitesi

    Kimya Mühendisliği Ana Bilim Dalı

    PROF. DR. ALİ KARADUMAN

  2. Plastik atıkların oksidatif ve inert ortamda ısıl ve katalitik bozunma ile karboksilli asitlere dönüşümü

    Thermal and catalytic degradation of plastic wastes into carboxylic acids in oxidative or inert media

    ADİL KOÇ

    Doktora

    Türkçe

    Türkçe

    2003

    Kimya MühendisliğiAnkara Üniversitesi

    Kimya Mühendisliği Ana Bilim Dalı

    PROF. DR. Y. ALİ BİLGESÜ

  3. Catalytic pyrolysis of plastic wastes over SAPO-34 catalyst

    Plastik atıkların SAPO-34 katalizörü üzerinde katalitik pirolizi

    TÜLAY BURSALI

    Yüksek Lisans

    İngilizce

    İngilizce

    2014

    Kimya MühendisliğiOrta Doğu Teknik Üniversitesi

    Kimya Mühendisliği Ana Bilim Dalı

    DOÇ. DR. NAİME ASLI SEZGİ

    PROF. DR. TİMUR DOĞU

  4. Plastik atıkların kimyasal bozundurma ile faydalı ürünlere dönüşümü için katalizör geliştirilmesi

    Developing catalysts for conversion of plastic wastes to useful products with chemical recycling

    SUZAN ALAN KORUN

    Yüksek Lisans

    Türkçe

    Türkçe

    2019

    Kimya Mühendisliğiİnönü Üniversitesi

    Kimya Mühendisliği Ana Bilim Dalı

    DR. ÖĞR. ÜYESİ ADİL KOÇ

  5. Polimetilmetakrilat (PMMA) plastik atıkların katalitik pirolizi

    Catalytic pyrolysis of polymethylmethacrylate (PMMA) plastic waste

    NEVİN SAYDAM

    Yüksek Lisans

    Türkçe

    Türkçe

    2012

    Kimya MühendisliğiAnkara Üniversitesi

    Kimya Mühendisliği Ana Bilim Dalı

    PROF. DR. ALİ KARADUMAN