Geri Dön

Sülfatlı zeminlerde yüksek fırın cürufu kullanılarak oluşturulan derin karıştırma kolonlarının rijitlik, geçirimlilik ve dayanım özelliklerinin araştırılması

Investigation of the stiffness, permeability and strength of deep mixing columns installed with blast furnace slag in sulfate bearing soils

  1. Tez No: 1030623
  2. Yazar: ALİCAN ŞENKAYA
  3. Danışmanlar: PROF. DR. MURAT OLGUN
  4. Tez Türü: Doktora
  5. Konular: İnşaat Mühendisliği, Civil Engineering
  6. Anahtar Kelimeler: Belirtilmemiş.
  7. Yıl: 2026
  8. Dil: Türkçe
  9. Üniversite: Konya Teknik Üniversitesi
  10. Enstitü: Lisansüstü Eğitim Enstitüsü
  11. Ana Bilim Dalı: İnşaat Mühendisliği Ana Bilim Dalı
  12. Bilim Dalı: Geoteknik Mühendisliği Bilim Dalı
  13. Sayfa Sayısı: Belirtilmemiş.

Özet

Derin Karıştırma Yöntemi (DKY), özellikle ince taneli zeminlerde taşıma gücünü artırmak ve oturmaları azaltmak için sıklıkla kullanılan zemin iyileştirme yöntemlerinden biridir. Özellikle kurak iklimlerde ve yeraltı su hareketlerinin yoğun olduğu bölgelerde sülfat içeren zeminlerle sıkça karşılaşılmaktadır. Bu nedenle, sülfat içeren zeminlerde oluşturulan yüksek modüllü zemin elemanlarının dayanıklılığını sağlamak önemli bir tasarım kriteri haline gelmiştir. DKY ile oluşturulan Derin Karıştırma Kolonu (DKK)'nun ana malzemesi sülfat içeren zeminin kendisidir. Sülfatın sadece dış etken değil, zemin biriminin bir parçası olması çözümü karmaşıklaştırmaktadır. Bu çalışmada, sülfat içeren killi zeminlerde oluşturulan DKK elemanlarının dayanıklılığını artırmak için CEM I 42.5 R çimentosuna ikame olarak yüksek fırın cürufu (YFC) kullanılmıştır. Kullanılan ince taneli zemin, doğal olarak sülfat içeren bir araziden elde edilmiştir. Deney tasarımı, Merkezi Kompozit Tasarım (MKT) yöntemi kullanılarak yapılmıştır. Her bir tasarım dört ayrı ve eşdeğer grup halinde üretilmiştir. Bu numune gruplarının üçü 120, 180 ve 360 gün boyunca %2'lik MgSO4 çözeltisine maruz bırakılmış; kontrol grubu numuneleri ise 360 gün boyunca saf suda bekletilmiştir. Her bir maruziyet döneminin sonunda; serbest basınç dayanımı (UCS), konsolidasyonsuz drenajsız üç eksenli basınç dayanımı (UU) ve geçirimlilik deneyleri yapılmıştır. Bu deneylerden; serbest basınç dayanımı (qu), drenajsız kohezyon (cuu), tanjant modülü (E50) ve boşaltma-yeniden yükleme modülü (Eur) ve geçirimlilik katsayısı (k) parametreleri elde edilmiştir. Her bir parametre ve maruziyet koşulu için ayrı ayrı istatistik analizler Yanıt Yüzey Yöntemi (YYY) kullanılarak yapılmıştır. Her bir istatistik analizden bir model denklemi kurulmuştur ve bu denkleme göre üç boyutlu yüzey grafikleri çizilmiştir. Sonuçlar kurulan bu istatistik modeller üzerinden yorumlanmıştır. Farklı sürelerde MgSO4 maruziyetinin elde edilen tüm parametreler üzerindeki etkileri irdelenmiştir. Optimum tasarım parametreleri 360 gün MgSO4 maruziyeti sonuçlarına göre belirlenmiştir. Optimum tasarım ve seçilen diğer iki tasarıma göre küçük ölçekli model DKK elemanlar üretilmiştir. Bu model kolonlardan elde edilen karot numuneleri iki gruba ayrılarak 360 gün MgSO4 çözeltisine ve saf suya maruz bırakılmıştır. Laboratuvar numuneleri ile küçük ölçekli DKK kolonlarının sonuçları kıyaslanmıştır. Seçilen numunelerin X-ışını kırınımı (XRD) ve taramalı elektron mikroskobu (SEM) analizleri yapılarak sülfatın etkileri mikroyapı analizleri açısından da irdelenmiştir. Buna göre YFC kullanımı, MgSO4 etkisi olmayan kontrol numunelerinde düzenli bir iyileşme eğilimi yaratırken; MgSO4 maruziyeti durumunda iyileşme YFC oranı ile paralel değildir ve bir optimum YFC oranı söz konusudur.

Özet (Çeviri)

Deep Soil Mixing (DSM) is one of the most widely used ground improvement methods for increasing bearing capacity and reducing settlement, particularly in fine-grained soils. Sulfate-bearing soils are frequently encountered in arid regions and areas with intense groundwater movement. Therefore, ensuring the durability of high-modulus soilcrete elements constructed in sulfate-bearing soils has become an important design criterion. Since the primary material of Deep Mixing Columns (DMCs) is the sulfate-bearing soil itself, sulfate acts not only as an external agent but also as an inherent component of the ground, making the problem more complex. In this study, ground granulated blast-furnace slag (GGBFS) was used as a partial replacement for CEM I 42.5 R cement to improve the durability of DMCs constructed in sulfate-bearing clay. The fine-grained soil was obtained from a naturally sulfate-bearing site. The experimental program was designed using the Central Composite Design (CCD) method. Each mix design was produced in four identical groups. Three groups were exposed to a 2% MgSO₄ solution for 120, 180, and 360 days, while the control group was stored in distilled water for 360 days. At the end of each exposure period, unconfined compressive strength (UCS), unconsolidated-undrained triaxial compression (UU), and permeability tests were performed. The measured parameters included unconfined compressive strength (qu), undrained cohesion (cuu), tangent modulus (E50), unloading-reloading modulus (Eur), and coefficient of permeability (k). Response Surface Methodology (RSM) was applied separately to each parameter and exposure condition. Statistical models were established, and three-dimensional response surface plots were generated to interpret the results. The effects of different MgSO₄ exposure durations on all measured parameters were evaluated. Optimum design parameters were determined based on the results after 360 days of MgSO₄ exposure. Small-scale DMC specimens were then produced using the optimum design and two additional selected mixtures. Core samples obtained from these model columns were divided into two groups and exposed to either a MgSO₄ solution or distilled water for 360 days. The results of the laboratory specimens and the model DMCs were compared. X-ray diffraction (XRD) and scanning electron microscopy (SEM) analyses were conducted on selected specimens to investigate the microstructural effects of sulfate attack. The results showed that GGBFS provided a consistent improvement in the control specimens without MgSO₄ exposure, whereas under MgSO₄ exposure the improvement was not proportional to the GGBFS content, indicating the existence of an optimum GGBFS replacement ratio.

Benzer Tezler

  1. Pik demiri ve karbon çeliğinin sulu çözeltiler içindeki korozyon hızının tayini

    Determination of the rate of corrosion of the cast iran and carbon steel in the aqueous solutions

    EMİNE NAZAN ÜNAL

    Yüksek Lisans

    Türkçe

    Türkçe

    1985

    Gazi Üniversitesi

    Kimya Mühendisliği Ana Bilim Dalı

    Yükleniyor...

  2. Manisa-Demirci-Köseler plaserinden titan minerallerinin kazanılması ve pigment üretimine katkı araştırmaları

    Recovery of the titanium minerals from Manisa-Demirci-Köseler plocer sands and examination of their use in prgment production

    SADULLAH ERTEKİN

    Yüksek Lisans

    Türkçe

    Türkçe

    1985

    Gazi Üniversitesi

    Kimya Mühendisliği Ana Bilim Dalı

    Yükleniyor...

  3. Düşük tenörlü pirolüzit cevherlerinden yeni bir MnSO4-H2O üretim metodu

    Başlık çevirisi yok

    MAHMUT BAYRAMOĞLU

    Doktora

    Türkçe

    Türkçe

    1983

    İstanbul Üniversitesi

    Kimya Mühendisliği Bilim Dalı

    Yükleniyor...

  4. Kütahya Gümüşköy-Aktepe baritinin flotasyonla zenginleştirilmesi

    Başlık çevirisi yok

    BAHRİ ÖTEYAKA

    Yüksek Lisans

    Türkçe

    Türkçe

    1985

    Anadolu Üniversitesi

    Yükleniyor...