Geri Dön

EDTA kompleksleştirici tuzu kullanılarak kimyasal depolama yöntemi ile MnS ince filmlerin elde edilmesi ve fiziksel özelliklerinin incelenmesi

Obtaining MnS thin films by chemical bath deposited method using EDTA complexing salt and the investigation of their physical properties

  1. Tez No: 771966
  2. Yazar: CANSU KARAKOYUN
  3. Danışmanlar: DOÇ. DR. CEMAL ULUTAŞ
  4. Tez Türü: Yüksek Lisans
  5. Konular: Fizik ve Fizik Mühendisliği, Physics and Physics Engineering
  6. Anahtar Kelimeler: EDTA, Gamma MnS, İnce Film, Kimyasal Depolama Yöntemi, Yapısal Özellik, Optiksel Özellik, Gama ışınları, Kimyasal depolama, Optik özellikler, Yapısal özellikler, İnce filmler, EDTA, Gamma MnS, Thin Film, Chemical Bath Deposited Method, Structural Properties, Optical Properties, Gamma rays, Chemical deposition, Thin films
  7. Yıl: 2022
  8. Dil: Türkçe
  9. Üniversite: Hakkari Üniversitesi
  10. Enstitü: Lisansüstü Eğitim Enstitüsü
  11. Ana Bilim Dalı: Fizik Ana Bilim Dalı
  12. Bilim Dalı: Belirtilmemiş.
  13. Sayfa Sayısı: Belirtilmemiş.

Özet

Bu çalışmada, 0.2 M EDTA kullanılarak MnS ince filmleri 5-10-15 saat sürelerde kimyasal depolama yöntemi (CBD) kullanılarak 40 oC sıcaklıkta cam alttaban üzerinde hazırlandı. Filmlerin yapısal, optiksel ve elektriksel özellikleri araştırıldı. Filmlerin karekterizasyonu X-ışını kırınımı (XRD), alan etkili taramalı elektron mikroskobu (FESEM), X-ışınları analizi (EDX), UV-vis spektrofotometresi ve Hall ölçümü sistemleri kullanılarak yapıldı. XRD analizlerinden filmlerin hegzegonal fazda polikristal yapıda büyüdüğü görüldü. EDX analizlerinden filmlerin stokyometrik oluştuğu görüldü. Optiksel sabitler olan sönüm katsayısı (k), kırılma indisi (n), dielektrik sabitinin gerçek (ε1) ve imajiner (ε2) kısmı ile filmin yasak enerji aralıkları (Eg) daldırma sürelerine bağlı olarak olarak incelendi. Filmlerin n tipi olduğu görülmüş olup daldırma sürelerine bağlı olarak özdirençleri 4.65-13.4x105 (Ω cm) aralığında ölçüldü.

Özet (Çeviri)

In this study, MnS thin films were prepared using 0.2 M EDTA for 5-10-15 hours on glass substrate at 40 oC using Chemical Bath Deposited Method (CBD). Structural, optical and electrical properties of the films were investigated. The characterization of the films were performed using X-ray diffraction (XRD), field effect scanning electron microscopy (FESEM), X-ray analysis (EDX), UV-vis spectrophotometer and Hall measurement systems. XRD analyzes showed that the films grew in a polycrystalline structure in the hexagonal phase. It was seen from the EDX analyzes that the films were formed stoichiometrically. The optical constants such as extinction coefficient (k), refractive index (n), real (ε1) and imaginary (ε2) parts of the dielectric constant and forbidden energy gaps (Eg) of the film were investigated depending on the immersion times. It was seen that the films were n-type and their resistivity was measured in the range of 4.65-13.4x105 (Ω cm) depending on the immersion time.

Benzer Tezler

  1. Molibdenitten amonyumheptamolibdat ve molibdenoranj üretimi

    Başlık çevirisi yok

    NURAY BAŞGÖL

    Yüksek Lisans

    Türkçe

    Türkçe

    1984

    İstanbul Üniversitesi

    Kimya Ana Bilim Dalı

    Yükleniyor...

  2. Hidrate bor minerallerinin termik özellikleri

    Başlık çevirisi yok

    SABRİYE PİŞKİN

    Doktora

    Türkçe

    Türkçe

    1983

    İstanbul Teknik Üniversitesi

    Yükleniyor...

  3. Proteinlerin ısı ile denatürasyonuna etilen diamin tetra asetik asit tetra sodyum tuzu (EDTA)'nun etkisinin incelenmesi

    Başlık çevirisi yok

    YASEMİN DEMİROĞLU

    Tıpta Uzmanlık

    Türkçe

    Türkçe

    1988

    İstanbul Üniversitesi

    Biyokimya Ana Bilim Dalı

    Yükleniyor...

  4. Anot çamurundaki selenin polarografik tayini için yöntem geliştirilmesi

    Başlık çevirisi yok

    ERDOĞAN HASDEMİR

    Doktora

    Türkçe

    Türkçe

    1988

    Hacettepe Üniversitesi

    Kimya Ana Bilim Dalı

    Yükleniyor...