Farklı üretim teknolojileri (SLA ve DLP) ve baskı yönelimlerinin eklemeli imalatla üretilen daimi rezin materyallerinin yüzey pürüzlülüğü ve bağlanma dayanımı üzerindeki etkisinin değerlendirilmesi
Evaluation of the effects of different printing technologies (SLA and DLP) and printing orientations on the surface roughness and bond strength of additively manufactured permanent resin-based materials
- Tez No: 1027807
- Danışmanlar: PROF. DR. ESMA BAŞAK GÜL AYGÜN
- Tez Türü: Diş Hekimliği Uzmanlık
- Konular: Diş Hekimliği, Dentistry
- Anahtar Kelimeler: 3B baskı, daimi rezin esaslı materyal, stereolitografi, dijital ışık işleme, yüzey pürüzlülüğü, makaslama bağlanma dayanımı, 3D printing, permanent resin-based material, stereolithography, digital light processing, surface roughness, shear bond strength
- Yıl: 2026
- Dil: Türkçe
- Üniversite: Çukurova Üniversitesi
- Enstitü: Diş Hekimliği Fakültesi
- Ana Bilim Dalı: Protetik Diş Tedavisi Ana Bilim Dalı
- Bilim Dalı: Protetik Diş Tedavisi Bilim Dalı
- Sayfa Sayısı: Belirtilmemiş.
Özet
Amaç: Bu in vitro çalışmanın amacı, iki farklı üretim teknolojisi (SLA ve DLP) ve üç farklı baskı yönelimi (0°, 45°, 90°) ile üretilen daimi rezin esaslı 3B baskı materyalinin yüzey pürüzlülüğü ve bir rezin simanla elde edilen makaslama bağlanma dayanımı (SBS) üzerindeki etkilerini karşılaştırmalı olarak değerlendirmektir. Gereç ve Yöntem: Çalışmada, aynı daimi rezin esaslı 3B baskı materyali kullanılarak SLA ve DLP teknolojileri ile toplam 210 adet disk şeklinde örnek üretildi. Örnekler 0°, 45° ve 90° baskı yönelimlerine göre alt gruplara ayrıldı. Numunelerin yüzey pürüzlülüğü optik profilometre ile değerlendirildi ve seçilmiş örneklerde SEM analizi yapıldı. Tüm örneklere standart kumlama işlemi uygulandıktan sonra primer ve self-adeziv rezin siman kullanılarak simantasyon gerçekleştirildi. Makaslama bağlanma dayanımı testi üniversal test cihazında 1 mm/dk çapraz kafa hızında yapıldı. Kırılma tipleri stereomikroskop altında incelendi. Veriler iki yönlü ANOVA, Mann-Whitney U testi ve Kruskal-Wallis testi ile analiz edildi; çoklu karşılaştırmalarda Bonferroni düzeltmesi uygulandı (p<0,05). Bulgular: Yüzey pürüzlülüğü açısından üretim teknolojileri arasında anlamlı fark bulunmazken, en yüksek pürüzlülük değerlerinin 45° baskı yöneliminde elde edildiği belirlendi (p<0,001). SLA grubunda ortalama SBS değeri 11,243±5,568 MPa, DLP grubunda ise 12,596±5,010 MPa olarak bulundu ve gruplar arasındaki fark istatistiksel olarak anlamlıydı (p=0,027). Baskı yöneliminin SBS üzerinde anlamlı etkisi saptanmadı (p=0,492). En sık görülen kırılma tipi koheziv kırılma olarak saptandı. Sonuç: Bu çalışma koşullarında, üretim teknolojisinin yüzey pürüzlülüğü üzerindeki etkisi anlamlı bulunmamıştır. Buna karşın, baskı yöneliminin yüzey pürüzlülüğünü etkilediği ve en yüksek yüzey pürüzlülüğü değerlerinin 45° baskı yöneliminde elde edildiği belirlenmiştir. SLA teknolojisi ile üretilen örneklerle karşılaştırıldığında, DLP teknolojisi ile üretilen daimi rezin esaslı 3B baskı materyallerinin daha yüksek makaslama bağlanma dayanımı gösterdiği saptanmıştır. Baskı yöneliminin ise bağlanma dayanımı üzerinde anlamlı bir etkisi bulunmamıştır.
Özet (Çeviri)
Objective: The aim of this in vitro study was to comparatively evaluate the effects of two different printing technologies, stereolithography (SLA) and digital light processing (DLP), and three different printing orientations (0°, 45°, and 90°) on the surface roughness and shear bond strength (SBS) to a resin cement of a permanent resin-based 3D printing material. Materials and Methods: A total of 210 disk-shaped specimens were produced using the same permanent resin-based 3D printing material with SLA and DLP technologies. The specimens were divided into subgroups according to the printing orientations of 0°, 45°, and 90°. Surface roughness was evaluated using an optical profilometer, and selected specimens were analyzed by scanning electron microscopy. After standardized airborne- particle abrasion, cementation procedures were performed using a primer and a self- adhesive resin cement. Shear bond strength tests were carried out in a universal testing machine at a crosshead speed of 1 mm/min. Failure modes were examined under a stereomicroscope. The data were analyzed using Two-Way ANOVA, Mann–Whitney U test, and Kruskal–Wallis test; Bonferroni correction was applied for multiple comparisons (p<0.05). Results: No significant difference was found between the production technologies in terms of surface roughness, whereas the highest roughness values were obtained at the 45° printing orientation (p<0.001). The mean SBS value was 11.243±5.568 MPa in the SLA group and 12.596±5.010 MPa in the DLP group, and the difference was statistically significant (p=0.027). Printing orientation did not significantly affect SBS values (p=0.492). Cohesive failure was the most common failure type in all groups. Conclusion: Under the conditions of this study, the effect of production technology on surface roughness was not statistically significant. In contrast, printing orientation affected surface roughness, and the highest surface roughness values were observed at the 45° printing orientation. In addition, permanent resin-based 3D printing materials produced with DLP technology showed higher shear bond strength than those produced with SLA technology. Printing orientation did not have a significant effect on bond strength.
Benzer Tezler
- Farklı 3D baskı reçinelerle üretilen implantüstü daimi kronların üretim doğruluğu, marjinal uyum ve iç uyumu açısından karşılaştırılması
Comparison of implant-supported permanent crowns produced with different 3D printed resins in terms of production accuracy, marginal fit and internal fit
TUĞBA HERGÜNER
- 3 boyutlu baskı teknolojileri ile üretilen farklı dental model tasarımlarının boyutsal özelliklerinin karşılaştırılması
Comparison of dimensional properties of different dental model designs manufactured with 3D printing technologies
EBRU YURDAKURBAN
- Dijital dental modeller kullanılarak 3 boyutlu yazıcıların doğruluğunun ve güvenilirliğinin karşılaştırılması
Comparison of the accuracy and relability of 3D printers using digital dental models
ŞULE GÖKMEN
- Üç boyutlu yazıcı ile üretilen rezin bazlı geçici kuron materyallerine uygulanan Parylene C nanoyüzey kaplama işleminin materyalin yüzey pürüzlülüğüne, ıslanabilirliğine ve Kandida tutulumuna etkisinin değerlendirilmesi
Evaluation of the effects of Parylene C nanosurface coating on surface roughness, wettability, and Candida albicans adhesion of 3Dprinted resin based temporary crown materials
CEYLAN SADİOĞLU AKDOĞAN
Diş Hekimliği Uzmanlık
Türkçe
2025
Sağlık Bilimleri ÜniversitesiProtetik Diş Tedavisi Ana Bilim Dalı
Yükleniyor...
- Farklı 3B yazıcı teknolojisi kullanılarak üretilen geçici restorasyon materyallerinin mekanik özelliklerinin incelenmesi
Evaluation of mechanical properties of temporary restoration materials produced using different 3D printer technologies
MEHMET ÜNAL
Diş Hekimliği Uzmanlık
Türkçe
2024
Çukurova ÜniversitesiProtetik Diş Tedavisi Ana Bilim Dalı
Yükleniyor...