Farklı tanecik büyüklüğüne sahip kobalt-krom alaşım tozundan eklemeli üretim yöntemiyle elde edilmiş metal altyapıların porselen bağlantı dayanımının incelenmesi
Investigation of the porcelain bond strength of metal frameworks obtained by additive manufacturing using Co-Cr alloy powders with different particle sizes
- Tez No: 1028579
- Danışmanlar: DOÇ. DR. HAYDAR ALBAYRAK
- Tez Türü: Diş Hekimliği Uzmanlık
- Konular: Diş Hekimliği, Dentistry
- Anahtar Kelimeler: Metal-Seramik Restorasyon, Üretim stratejisi, Bağlantı Dayanımı, EDS, XRD, Metal–Ceramic Restoration, Manufacturing Strategy, Bond Strength, EDS, XRD
- Yıl: 2026
- Dil: Türkçe
- Üniversite: Erciyes Üniversitesi
- Enstitü: Diş Hekimliği Fakültesi
- Ana Bilim Dalı: Protetik Diş Tedavisi Ana Bilim Dalı
- Bilim Dalı: Protetik Diş Tedavisi Bilim Dalı
- Sayfa Sayısı: Belirtilmemiş.
Özet
Günümüzde metal seramik (MS) restorasyonların altyapılarının üretiminde seçici lazer ergitme (SLE) yöntemi rutin olarak kullanılmaktadır. Bu çalışmanın amacı, iki farklı tanecik (10-30µ; Grup-30, 15-45µ;Grup-45) büyüklüğüne sahip aynı içerikli Co-Cr tozundan iki farklı üretim parametreleri (Grup-P1, Grup-P2) kullanılarak üretilmiş numunelerin porselen bağlantı dayanımlarının karşılaştırılmasıdır. Toplamda 40 bar (25mmx3mmx0,5mm) şekilli ve 4 kare(20mmx20mmx1mm) şekilli Co-Cr altyapı SLE yöntemi ile üretilmiştir. Daha sonra bar şekilli altyapılara porselen uygulandı (Uluslararası Standartlar Organizasyonunun 9693) ve fırınlandı. Tüm bar şekilli numunelere üç nokta bükme testi uygulanmış ve MS bağlantı dayanım değerleri hesaplanmıştır (MPa). Üç nokta bükme testinin ardından, her gruptan rastgele seçilen bir numunenin kırık ara yüzeyleri stereomikroskop ve taramalı elektron mikroskobu (SEM) ile incelendi, enerji dağılımlı X-ışını spektroskopisi (EDS) kullanılarak analiz edildi. Kare şekilli numunelerin mikro yapısı X-Işını diffraksiyon yöntemi ile değerlendirildi. Veriler, iki yönlü varyans analizi ile değerlendirildi. Grup P2 (29.4±2.63) grup P1'den (25.94±3.01) istatistiksel olarak anlamlı derece yüksek MS bağlantı dayanımı sergilemiştir (P<0.001). Tanecik büyüklüğü ile parametre etkileşimi istatistiksel olarak anlamlıdır (P=0.008361). P2-45 (29,81±2,33) P1 45'ten (24,1±3,09), P1-30 (27,78±1,45) P1-45'ten istatistiksel olarak anlamlı derecede yüksek MC bağlantı değeri sergilemiştir. Kırık ara yüzeyler benzer element içeriğine sahipti. Tüm metal altyapılar benzer X-Işını kırınım deseni sergiledi. Bu çalışmada P1-45 etkileşimi hariç gruplar ISO 9693 standartlarına göre klinik olarak uygulanabilir özelliktedir. MS altyapı üretiminde kullanılan SLM parametreleri MS bağlantı dayanımını etkilerken, kullanılan alaşım tozunun tanecik büyüklüğü MS bağlantı dayanımını etkilememiştir. 15–45 µm tanecik boyutunda Parametre 2 önerilirken, Parametre 1 yalnızca 10–30 µm tanecik boyutu ile kullanılmalıdır.
Özet (Çeviri)
Selective laser melting (SLM) technique is currently routinely used for the fabrication of frameworks for metal–ceramic (MC) restorations. The aim of this study was to compare the porcelain bond strengths of frameworks fabricated using Co–Cr powders of identical composition with two different particle-size ranges (10–30 µm, Group 30; and 15–45 µm, Group 45) and two different manufacturing parameters (Group P1 and Group P2). A total of 40 bar-shaped Co–Cr frameworks (25 mm × 3 mm × 0.5 mm) and four square-shaped Co–Cr frameworks (20 mm × 20 mm × 1 mm) were manufactured using the SLM technique. Porcelain was subsequently applied to all bar-shaped frameworks in accordance with International Organization for Standardization (ISO) 9693 and fired. All bar-shaped specimens were subjected to a three-point bending test, and the MC bond strength values were calculated (MPa). Following the bending test, the fractured bonding interfaces of one randomly selected specimen from each group were examinated using stereomicroscopy and scanning electron microscopy (SEM), analized using energy-dispersive X-ray spectroscopy (EDS). The microstructures of the square-shaped specimens were examined using X-ray diffraction (XRD). The data were evaluated using two-way analysis of variance. Group P2 (29.4±2.63) showed statistically significantly higher MC bond strength than group P1 (25.94±3.01) (P<0.001). The interaction between particle size and parameter is statistically significant (P=0.008361). P2-45(29.81±2.33) showed a statistically significantly higher MC bond value than P1-45 (24.1±3.09), and P1-30 (27.78±1.45) showed a statistically significantly higher MC bond value than P1-45. The fractured interfaces were found to have similar elemental compositions. The metal frameworks exhibited similar X-ray diffraction patterns. In this study, all groups, except for the P1-45 interaction, demonstrated clinically acceptable properties according to ISO 9693. The SLM processing parameters used for the fabrication of metal–ceramic (MC) frameworks affected the metal–ceramic bond strength, whereas the particle size of the Co–Cr alloy powder did not. Parameter 2 is recommended for the 15–45 µm particle-size range, while Parameter 1 should only be used with the 10–30 µm particle-size range.
Benzer Tezler
- Bazı esterlerin kinetik incelenmesi ve termodinamik parametrelerin belirlenmesi
Kinetic study and detesmination of thermodnamic parameters of some esters
İBRAHİM TAŞ
- İzmir'de bazı yolların kapatılarak yaya bölgeleri oluşturma da kent peyzajını geliştirme açısından yeniden planlanması üzerinde araştırmalar
Başlık çevirisi yok
BAHAR TÜRKYILMAZ
- Testosteron dihidrotestosteron ve östrojenin benign prostat hiperplazisindeki etyolojik rolleri
The roles of testosterone, dihydrotestosterone and estradiole on the etiology of benign prostatic hyperplasia
HALUK TOKUÇOĞLU
- Süt formüllerinin tüketim uygulamaları ve süt formüllerinin C vitamini içeriği ile pH değerleri
Başlık çevirisi yok
GÖNÜL VAROL