CAD/CAM teknolojisi ile üretilen farklı tam seramik kron restorasyonların internal ve marjinal uyumları ile klinik başarılarının in vivo olarak değerlendirilmesi

In vivo evaluation of the internal and marginal adaptation and clinical success of different full ceramic crowns generated with CAD/CAM technology

  1. Tez No: 479127
  2. Yazar: SİNEM OK
  3. Danışmanlar: PROF. DR. YASEMİN ÖZKAN
  4. Tez Türü: Doktora
  5. Konular: Diş Hekimliği, Dentistry
  6. Anahtar Kelimeler: CAD/CAM, tam-seramik, marjinal uyum, internal uyum, Dental estetik, Dental materyaller, Dental porselen, Dental restorasyon, Dental çimentolar, CAD/CAM, all-ceramic, marginal fit, internal fit, Dental aesthetics, Dental materials, Dental porcelain, Dental restoration, Dental cements
  7. Yıl: 2017
  8. Dil: Türkçe
  9. Üniversite: Marmara Üniversitesi
  10. Enstitü: Sağlık Bilimleri Enstitüsü
  11. Ana Bilim Dalı: Protetik Diş Tedavisi Ana Bilim Dalı
  12. Bilim Dalı: Belirtilmemiş.
  13. Sayfa Sayısı: Belirtilmemiş.

Özet

Amaç: Bu çalışmanın amacı, CAD/CAM teknolojisiyle üretilen farklı yapıdaki tam seramik kron restorasyonların simantasyon öncesi marjinal ve internal uyumlarının karşılaştırılması ve tedavinin başlangıcı ile simantasyondan 6 ay sonraki klinik sonuçların karşılaştırılmasıdır. Gereç ve yöntem: 15 adet lityum disilikat seramik kron (LDS, IPS e.max CAD Blocks, Ivoclar, Vivadent, Schaan, Liechtenstein) ve 30 adet lityum disilikat ile güçlendirilmiş lityum alüminosilikat cam-seramik kron (LAS, n!ce® CAD Blocks, Institut Straumann AG, Basel, Switzerland) olmak üzere 45 adet tam seramik kron 38 hastaya uygulanmıştır. Kronların marjinal ve internal aralık değerlerini ölçmek için silikon replika tekniği kullanılmıştır. Silikon replikalar bukko-lingual ve mesio-distal olmak üzere kesitlendirilip ışık mikroskobu ile (40 magnifikasyon) değerlendirilmiştir. Her diş için 20 referans noktası belirlenerek ölçümlenmiş ve ortalama marjinal ve internal aralıklar kaydedilmiştir. Restorasyonlar, tedavinin başlangıcında ve simantasyondan 6 ay sonra USPHS kriteri, kanama ve plak indeksi ve hasta memnuniyeti kriterlerine göre değerlendirilmiştir. İlgili veriler“Mann-Whitney U”ve“Wilcoxon Signed Rank”testleri kullanılarak analiz edilmiştir (P<0.05). Bulgular: 6 aylık gözlem sürecinden sonra LDS ve LAS gruplarının toplam başarı oranı %100 olarak belirlenmiştir. Ortalama marjinal aralıklar, LDS grubu için 53.30 (± 11.27) μm, LAS grubu için 51.67 (± 11.24) μm olarak hesaplanmıştır. En büyük değer oklüzal alanda (LDS= 152,24 ± 20,27 μm, LAS= 154,66 ± 23,46 μm), en düşük değeri ise aksiyal (LDS=58,08 ±14,59μm, LAS= 46,73 ± 10,72 μm) alanda gözlemlenmiştir (P<0.05). Sonuç: Ortalama 6 aylık değerleme süresinde LDS ve LAS tam seramik kronlardan elde edilen veriler literatür kriterlerine göre kabul edilebilir sınırlar içerisindedir.

Özet (Çeviri)

Purpose: The aims of this clinical study were to compare the marginal and internal adaptation of all-ceramic crowns generated with CAD/CAM before cementation and examine the clinical outcomes at baseline and 6th month after luting. Materials and methods: All crowns were placed in 38 patients, including 15 lithium disilicate ceramic crowns (LDS, IPS e.max CAD Blocks, Ivoclar, Vivadent, Schaan, Liechtenstein), 30 lithium disilicate stengthened lithium aluminosilicate glass-ceramic crowns (LAS, n!ce® CAD Blocks, Institut Straumann AG, Basel, Switzerland). The marginal and internal gaps of crowns were recorded by using a replica technique. The replica specimens were sectioned bucco-lingually and mesio-distally and the thickness of silicone layers was examined by computerized light microscope at × 40 magnification.. Restorations were clinically assessed at baseline and 6th after cementation by using modified USPHS criteria, plaque and gingival indexes and patients satisfaction criteria. Data was analysed by using“Mann-Whitney U”and“Wilcoxon Signed Rank”tests (P<0.05). Results: After 6 month-observation period, total survival rates of LDS and LAS groups were 100%. The mean marginal gaps were 53.30 (± 11.27) μm for LDS group and 51. 67 (± 11. 24) μm for LAS group. The highest gap value was observed at the occlusal area (LDS= 152.24 ± 20.27 μm, LAS= 154.66 ± 23.46 μm), and lowest one at the axial area (LDS=58.08 ±14.59μm, LAS= 46.73 ± 10.72 μm) (P<0,05). Conclusions: Regarding all of the clinical evaluation criteria all LDS and LAS crowns exhibited clinically acceptable scores within an average evaluation time of 6 months.

Benzer Tezler

  1. Aynı sisteme ait farklı bilgisayar destekli ölçü yöntemlerinin farklı restorasyonların uyumuna etkilerinin karşılaştırılması

    Comparison of the effects of different computer aided impressions belong the same system on different restorations' adaptation

    ZEYNEP EKİCİ

    Diş Hekimliği Uzmanlık

    Türkçe

    Türkçe

    2018

    Diş HekimliğiAnkara Üniversitesi

    Protetik Diş Tedavisi Ana Bilim Dalı

    PROF. DR. MEHMET ALİ KILIÇARSLAN

  2. CAD/CAM teknolojisi ile üretilen farklı tam seramik blokların çiğneme kuvveti altında mekanik dayanımının değerlendirilmesi

    Evaluation of the mechanical strength of different full ceramic blocks produced with CAD/CAM technology under chewing force

    ŞEVVAL ÖKSÜZ

    Diş Hekimliği Uzmanlık

    Türkçe

    Türkçe

    2024

    Diş HekimliğiEskişehir Osmangazi Üniversitesi

    Protetik Diş Tedavisi Ana Bilim Dalı

    PROF. DR. CANAN AKAY

  3. Farklı yüzey işlemleri uygulanan tek seans CAD/CAM blokların reçine simanı ile bağlantı dayanımının incelenmesi

    Farklı yüzey işlemleri uygulanan tek seans CAD/CAM blokların reçine simanı ile bağlantı dayanımının incelenmesi

    ŞEVKİ ÇINAR

    Doktora

    Türkçe

    Türkçe

    2018

    Diş Hekimliğiİstanbul Üniversitesi

    Protetik Diş Tedavisi Ana Bilim Dalı

    PROF. DR. GÖKHAN AKGÜNGÖR

  4. Farklı ağız gargaralarının güncel CAD/CAM materyallerinin optik özellikleri üzerine etkilerinin incelenmesi

    Investigation of the effects of different mouthwashes on the optical properties of current CAD/CAM materials

    GÖZDE YAVUZKILIÇ

    Diş Hekimliği Uzmanlık

    Türkçe

    Türkçe

    2025

    Diş HekimliğiOndokuz Mayıs Üniversitesi

    Protetik Diş Tedavisi Ana Bilim Dalı

    PROF. DR. GÖZLEM CEYLAN

  5. Üç farklı seramik üst yapı materyaline farklı yüzey işlemlerinin rezin simana yapışma direncinin saptanması

    Determination of different surface treatments adhesion resistance to resin cement applied to three different ceramic materials

    ASIM ÖZÜN

    Diş Hekimliği Uzmanlık

    Türkçe

    Türkçe

    2022

    Diş HekimliğiSüleyman Demirel Üniversitesi

    Protetik Diş Tedavisi Ana Bilim Dalı

    DOÇ. DR. HAKKI CENKER KÜÇÜKEŞMEN