Kendinden adezivli kompozit rezinlerin farklı universal adeziv sistemlerle birlikte uygulanarak mikrogerilim bağlantı dayanımlarının değerlendirilmesi
Mi̇crotensi̇le bond strengths of self-adhesi̇ve composi̇tes appli̇ed wi̇th uni̇versal adhesi̇ve systems
- Tez No: 549293
- Danışmanlar: DOÇ. DR. MURAT ÜNAL
- Tez Türü: Diş Hekimliği Uzmanlık
- Konular: Diş Hekimliği, Dentistry
- Anahtar Kelimeler: Kendinden Adezivli Kompozit, Universal Adeziv, Mikrogerilim Bağlanma Dayanımı Testi, SEM, Dental bonding, Dental materyaller, Dental restorasyon, Dental çimentolar, Kompozit reçineler, Mikroskopi-elektron taramalı, Self-adhesive composites, Universal Adhesive Systems, Micro-tensile bond strength, SEM, Dental bonding, Dental materials, Dental restoration, Dental cements, Composite resins, Microscopy-electron scanning
- Yıl: 2019
- Dil: Türkçe
- Üniversite: Sivas Cumhuriyet Üniversitesi
- Enstitü: Diş Hekimliği Fakültesi
- Ana Bilim Dalı: Çocuk Diş Hekimliği Ana Bilim Dalı
- Bilim Dalı: Belirtilmemiş.
- Sayfa Sayısı: Belirtilmemiş.
Özet
Çalışmamızın amacı, iki farklı kendinden adezivli kompozitin beş farklı universal adeziv sistem ile uygulanarak daimi diş dentinine bağlanma dayanımlarının in-vitro olarak değerlendirilmesidir. Çalışmada aynı renkte (A2) 2 farklı kendinden adezivli kompozit [Vertise™ Flow(VF), Fusio Liquid Dentin(FL)] ile 5 farklı universal bonding sistem (Clearfil Universal Bond, Single Bond Universal, All Bond Universal, Prime Bond Universal, Futurabond U) kullanıldı. Kendinden adezivli kompozitlerin direkt (kontrol grupları) ve beş farklı universal bond ile total-etch (TE) ve self-etch (SE) moduyla uygulandığı toplam 22 grup oluşturuldu. Toplam 48 adet çürüksüz insan molar dişi kullanılarak 240 adet mikrogerilim test çubuğu elde edildi. Her bir grubun örnek sayısı 10 olacak şekilde, universal test cihazında mikrogerilim test metodu ile incelenip, taramalı elektron mikroskobu ile değerlendirildi. Ayrıca gruplardaki bağlantı ve kırıklar SEM görüntülemesi ile incelendi. Veriler varyans analizi ve Tukey HSD testi ile istatistiksel olarak analiz edildi. Mikrogerilim testi sonucunda en yüksek bağlanma dayanımı VF grubunda Single Bond Universal adezivin total-etch modda kullanımında görülmüştür. En düşük bağlanma dayanımını ise FL kontrol grubunda göstermiştir. Kontrol grupları ile deney grupları arasındaki fark istatistiksel olarak önemli bulunmuştur(p<0.05). Kontrol gruplarında VF değerleri, FL grubuna göre yüksek bulundu ve istatistiksel olarak önemli bulundu(p<0.05).
Özet (Çeviri)
The aim of our study is to evaluate the dentine bonding strengths in vitro by applying two different self-adhesive composites with five different universal adhesive systems. In the study, 2 different self-adhesive composites [Vertise™ Flow(VF), Fusio Liquid Dentin(FL)] with the same color (A2) and 5 different universal bonding systems (Clear Bond Universal Bond, Single Bond Universal, All Bond Universal, Prime Bond Universal, Futurabond U) were used. A total of 22 groups were created in which self-adhesive composites were applied directly (control groups) and five different universal bond with total-etch and self-etch mode. A total of 48 human molar teeth were used for a total of 240 micro-tension test strips. The sample number of each group was determined as 10 and the samples were examined by microstring test method in universal test device and evaluated with scanning electron microscope (SEM). In addition, the connections and fractures in the groups were examined by SEM imaging. The data were analyzed statistically by variance analysis and Tukey HSD test. As a result of the micro-tension test, the highest bond strength was seen in the use of Single Bond Universal adhesive in the VF group in total-etch mode. The lowest bond strength was shown by the group in which the FL control group was applied without bonding. The difference between the control groups and the experimental groups was statistically significant (p <0.05). VF values in control groups were higher than FL group and statistically significant (p<0.05).
Benzer Tezler
- Küçük Yamanlar tepesi örneğinde kent yakın çevresinde rekreasyon alanı düzenleme projesi
Başlık çevirisi yok
NİHAN BULGUN
- 1985-1986 yıllarında Polatlı Devlet Hastanesine kaza nedeniyle başvuranların incelenmesi
Başlık çevirisi yok
FERHAN ŞENOL
Yüksek Lisans
Türkçe
1986
Gazi ÜniversitesiKazaların Çevresel ve Teknik Araştırması Ana Bilim Dalı (disiplinlerarası)
Yükleniyor...
- Antakya tarihi ticaret merkezi mekansal yapı değişim ve gelişim sürecinin kent ticaret merkezi planlamasına etkinliği
The Effectiveness of spatial structural chance and development period of the historical trade center of Antakya in the urban trade planning
NEVİN TURGUT