Geri Dön

Zirkonya alt yapılı porselen restorasyonların tamirinde endirekt faset uygulaması yöntemi ile direk tamir yönteminin bağlanma dayanımının, invitro olarak karşılaştırılması

An in vitro comparison of shear bond strength in indirect facet application method and direct repair method in zirconia-supported porcelain restorations

  1. Tez No: 671913
  2. Yazar: TUĞÇE MERVE ORDUERİ KILAVUZ
  3. Danışmanlar: PROF. DR. MEHMET MUZAFFER ATEŞ
  4. Tez Türü: Doktora
  5. Konular: Diş Hekimliği, Dentistry
  6. Anahtar Kelimeler: Dental bonding, Dental porselen, Dental restorasyon, Dental stres analizi, Zirkonyum, Dental bonding, Dental porcelain, Dental restoration, Dental stress analysis, Zirconium
  7. Yıl: 2021
  8. Dil: Türkçe
  9. Üniversite: İstanbul Medipol Üniversitesi
  10. Enstitü: Sağlık Bilimleri Enstitüsü
  11. Ana Bilim Dalı: Protetik Diş Tedavisi Ana Bilim Dalı
  12. Bilim Dalı: Belirtilmemiş.
  13. Sayfa Sayısı: Belirtilmemiş.

Özet

Bu çalışmanın amacı, zirkonya (Zr) alt yapılı restorasyonlarda karşılaşılan kırıkların, lamina veneerler ile indirekt ve kompozit sistemlerle yapılan direkt tamir yöntemlerinin bağlanma dayanımlarını karşılaştırmaktır. Çalışmada gruplar ağız içerisindeki porselen kırıklarını taklit edecek şekilde farklı porselen yüzdeleri ile oluşturuldu. Grup A = %100 Zr alan; Grup B= %70 Zr, %30 porselen alan; Grup C= %50 Zr, %50 porselen alan; Grup D= %30 Zr, %70 porselen alan; Grup E= %100 porselen alan, olmak üzere deney örnekleri hazırlandı. Grupların yarısına kompozit ile direk tamir, diğer yarısına porselen lamina veneer ile endirekt tamir yapıldı. Örnekler, yüzey işlemleri ve tamir uygulanmadan önce akrilik bloklara gömüldü. Sonrasında yüzey işlemlerini takiben, 1. gruplara lamina veneerler, 2. gruplara kompozit tamir sistemleri uygulandı. Tüm numuneler termal siklüs cihazında yaşlandırma işlemine tabii tutulduktan sonra, üniversal test cihazında bağlanma dayanımı değerlendirildi ve elde edilen veriler kayıt altına alındı. Örnekler stereomikroskop ile incelendi ve kırık tiplerine göre sınıflandırıldı (adeziv/ koheziv/ kombine). Bağlanma kuvveti verileri, bağımsız örnekler t testi ile değerlendirildi. Gruplar arasında, lamina ile yapılan tamirlerin bağlanma dayanımı, kompozit ile yapılan tamirlerden daha yüksek bulundu. İstatiksel olarak, Grup C hariç diğer bütün gruplarda endirekt tamir grupları lehine anlamlı fark bulundu. En yüksek bağlanma dayanımı Grup A da endirekt tamir yönteminde bulurken, en düşük bağlanma dayanımı Grup E de direkt tamir yönteminde bulundu. En çok adeziv kırık tipi kompozit ile tamir yapılan gruplarda görüldü.

Özet (Çeviri)

The aim of this study is to compare the bond strength of indirect repair method with laminate veneers and direct repair methods with composite systems in fractures of zirconia based porcelains. In the study, groups were formed with different porcelain percentages to imitate porcelain fractures in the mouth. The experimental samples were grouped as Group A= 100% Zr; Group B= 70% Zr, 30% porcelain surface; Group C= 50% Zr, 50% porcelain surface; Group D= 30% Zr, 70% porcelain surface; Group E= 100% porcelain surface. Half of which were repaired with composite and half of them were repaired with indirect facet method by porcelain laminate veneers. Samples were embedded in acrylic blocks before surface treatment and repair was applied. After the surface treatments, laminate veneers were applied to the 1st groups and composite repair systems to the 2nd groups. After all the samples were aged in the thermal cycle device, the bond strength was evaluated in the universal test device and the data obtained were recorded. Samples were examined with a stereomicroscope and classified according to fracture types (adhesive / cohesive / combined). Bond strength data were evaluated with independent t test statistics. Among the groups, the bond strength of repairs made with laminate veneer was higher than repairs made with composite. Statistically, there is a significant difference in favor of indirect repair groups in all groups except group C. The highest bond strength was found in the indirect repair method in group A, while the lowest bond strength was found in the direct repair method in group E. The most adhesive fracture type was seen in the composite groups.

Benzer Tezler

  1. Zirkonya esaslı seramik kaplamanın fiziksel ve kimyasal özelliklerinin değiştirilmesi

    Changing physical and chemical properties of zirconia based ceramic coating

    İSMET ÇEVİK

    Doktora

    Türkçe

    Türkçe

    1990

    İstanbul Teknik Üniversitesi

    Yükleniyor...

  2. Mullit-Zirkonya seramik kompozitlerinin reaksiyon sinterlemesi yöntemi ile elde edilmesi ve stransiyum oksit katkısısnın etkisi

    Başlık çevirisi yok

    SEHER KINIKOĞLU

    Doktora

    Türkçe

    Türkçe

    1993

    Yıldız Teknik Üniversitesi

    Metalurji Mühendisliği Ana Bilim Dalı

    Yükleniyor...

  3. Plazma sprey kaplamalarda bazı malzeme parametrelerinin bağlanma mukavemetine etkileri

    Başlık çevirisi yok

    MURAT DEMİRCİ

    Yüksek Lisans

    Türkçe

    Türkçe

    1994

    Marmara Üniversitesi

    Yükleniyor...

  4. A Study for the properties of zirconiq toughened alumina via statistical methods

    İstatistik yöntemlerle zirkonya toklandırılmış alumina özellikleri konusunda bir çalışma

    NUR ÖZKAN

    Yüksek Lisans

    İngilizce

    İngilizce

    1994

    Orta Doğu Teknik Üniversitesi

    Metalurji Mühendisliği Ana Bilim Dalı

    Yükleniyor...