Koyulhisar sfalerit konsantresinin asidik ferrik klorürlü ortamda liçing şartlarının belirlenmesi
Determination of leaching conditions of Koyulhisar sphalerite concentrate in acidic ferric chloride medium
- Tez No: 134158
- Danışmanlar: YRD. DOÇ. DR. SALİH AYDOĞAN
- Tez Türü: Yüksek Lisans
- Konular: Maden Mühendisliği ve Madencilik, Mining Engineering and Mining
- Anahtar Kelimeler: Belirtilmemiş.
- Yıl: 2003
- Dil: Türkçe
- Üniversite: Selçuk Üniversitesi
- Enstitü: Fen Bilimleri Enstitüsü
- Ana Bilim Dalı: Maden Mühendisliği Ana Bilim Dalı
- Bilim Dalı: Belirtilmemiş.
- Sayfa Sayısı: 63
Özet
ÖZET Yüksek Lisans Tezi KOYULHİSAR SFALERİT KONSANTRESİNİN ASİDİK FERRİK KLORÜRLÜ ORTAMDA LİÇİNG ŞARTLARININ BELİRLENMESİ ALİ ARAŞ Selçuk Üniversitesi Fen Bilimleri Enstitüsü Maden Mühendisliği Anabilim Dalı Danışman : Yrd. Doç. Dr. Salih AYDOĞAN 2003, 54 Sayfa Jüri : Prof. Dr. M. Kemal GÖKAY Yrd. Doç. Dr. Salih AYDOĞAN Yrd. Doç. Dr. Alper ÖZKAN Bu tezde Sivas - Koyulhisar yöresinde bulunan Cu - Pb - Zn kompleks cevherinden flotasyon yoluyla zenginleştirilmiş sfalerit konsantresinin asidik ortamda ferrik iyonları etkisinde çözündürülme şartlan ve kinetiği araştırılmıştır. Fe+3 kaynağı olarak ferrik klorür (FeCI3.6HbO) kullanılmıştır. Deneyler, sıcak su banyosunda 1 lt'lik beherlerde karıştırma liçi yapılarak gerçekleştirilmiştir. Araştırmalarda; karıştırma hızı, Fe+3 derişimi, katı/sıvı oranı, sıcaklık ve tane boyutunun çinko çözünmesine olan etkisi incelenmiştir. İncelenen koşullarda elde edilen sonuçlara göre sfalerit konsantresinden ferrik iyonları etkisinde çinko çözünmesinin; karıştırma hızından hemen hemen bağımsız, Fe+3 derişimi ve sıcaklık ile doğru orantılı, katı sıvı/oranı ve tane iriliği ile ters orantılı olduğu tespit edilmiştir. 600 dev/dak karıştırma hızında, 1.0 M Fe+3 derişiminde, 10/500 g/ml katı/sıvı oranında, 80 ° C sıcaklıkta ve -212 um tane iriliğinde % 82 Zn çözünmesi sağlanmıştır. Kinetik değerlendirme sonucunda sfalerit konsantresinden ferrik iyonları etkisinde Zn çözünmesinin küçülen partikül modeli (1-(1-X) ) 'ne uyduğu belirlenmiştir. Buradan; aktivasyon enerjisi 46.13 kJ/mol hesaplanmıştır. Zn çözünmesinin ferrik iyonlarına bağımlılığının [Fe+3]0,42, katı/sıvı oranına bağımlılığının (katı/sıvı)0,48 olduğu tespit edilmiştir. Anahtar Kelimeler : Sfalerit, ferrik klorür, liçing, liçing kinetiği
Özet (Çeviri)
ABSTRACT MSc Thesis DETERMINATION OF LEACHING CONDITIONS OF KOYULHİSAR SPHALERITE CONCENTRATE IN ACIDIC FERRIC CHLORIDE MEDIUM ALİ ARAS Selçuk University Graduate School of Natural and Applied Sciences Department of Mining Engineering Supervisor : Assist. Prof. Dr. Salih AYDO?AN 2003, 54 Pages Jury : Prof. Dr. M. Kemal GÖKAY Assist. Prof. Dr. Salih AYDO?AN Assist. Prof. Dr. Alper ÖZKAN In this thesis, dissolution conditions and kinetics of sphalerite concentrate enriched through flotation of Sivas-Koyulhisar Cu-Pb-Zn complex ore in acidic medium with ferric ions were investigated. Ferric chloride (FeCİ3.6H20) was used as source of ferric ions. Experiments were carried out in 1 It vessel using hot bath by agitation leaching. Effects of stirring speed, Fe concentration, solid/liquid ratio, temperature and particle size on zinc dissolution were investigated. According to obtained results, it was determined that zinc dissolution from sphalerite concentrate with ferric ions is nearly independent from stirring speed, directly proportional by Fe3+ concentration and temperature, inversely proportional by solid/liquid ratio and particle size. 82 % of zinc dissolution was obtained at 600 rpm stirring speed, 1.0 M Fe concentration, 10/500 g/ml solid/liquid ratio, 80° C temperature and -212 um particle size. It was determined using kinetic evaluation that zinc dissolution from sphalerite concentrate with ferric ions is consistent with shrinking particle model (1-(1-X)1/3). Activation energy was calculated 46.13 kJ/mol. Zinc dissolution was expressed with [Fe3+]042 and (solid/liquid ratio)048. Keywords : Sphalerite, ferric chloride, leaching, leaching kinetics
Benzer Tezler
- Sfaleritin asidik potasyum dikromatlı (K2Cr2O7) ortamda çözündürülmesi
Dissolution of sphalerite in acidic potassium dichromate (K2Cr2O7) medium
İSMAİL DEDEMLİ
Yüksek Lisans
Türkçe
2008
Maden Mühendisliği ve MadencilikSelçuk ÜniversitesiMaden Mühendisliği Ana Bilim Dalı
DOÇ. DR. SALİH AYDOĞAN
- Evaluation of mineralization and chemistry of the Kurşunlu lead-zinc deposits (Koyulhisar-Sivas)
Başlık çevirisi yok
MUHANNAD R. ARAR
Yüksek Lisans
İngilizce
1990
Jeoloji MühendisliğiOrta Doğu Teknik ÜniversitesiJeoloji Mühendisliği Ana Bilim Dalı
PROF. DR. AYHAN ERLER
- Kurşunlu (Ortakent-Koyulhisar-Sivas) Pb-Zn-Cu yataklarının jeolojisi
Başlık çevirisi yok
ATİLLA ÖZGÜNEYLİOĞLU
- Aksu Köyü (Ortakent-Koyulhisar-Sivas) kuzey kesiminin metalojenik özellikleri
Başlık çevirisi yok
İSMAİL ŞAHİN
Yüksek Lisans
Türkçe
1998
Jeoloji MühendisliğiCumhuriyet ÜniversitesiJeoloji Mühendisliği Ana Bilim Dalı
PROF. DR. AHMET GÖKÇE
- Sisorta (Ortakent-Koyulhisar-Sivas) yöresi altın yatağının jeolojik ve jeokimyasal özellikleri
Geological and geochemical features of Sisorta (Ortakent-Koyulhisar-Sivas) gold deposit
ÇİĞDEM ŞAHİN DEMİR
Doktora
Türkçe
2015
Jeoloji MühendisliğiCumhuriyet ÜniversitesiJeoloji Mühendisliği Ana Bilim Dalı
PROF. DR. ALİ UÇURUM