Farklı dental simanların titanyum materyalinin olası korozyon riski ve makaslama bağ dayanımı üzerindeki etkisinin incelenmesi
Investigation of the effect of different dental cements on the potential corrosion risk and shear bond strength of titanium material
- Tez No: 1024273
- Danışmanlar: DOÇ. DR. SEZGİ CİNEL ŞAHİN
- Tez Türü: Diş Hekimliği Uzmanlık
- Konular: Diş Hekimliği, Dentistry
- Anahtar Kelimeler: titanyum, korozyon, dental siman, makaslama bağ dayanımı, iyon salınımı, Makaslama, İyon, titanium, corrosion, dental cement, shear bond strength, ion release, Shear, Ion
- Yıl: 2026
- Dil: Türkçe
- Üniversite: Pamukkale Üniversitesi
- Enstitü: Diş Hekimliği Fakültesi
- Ana Bilim Dalı: Protetik Diş Tedavisi Ana Bilim Dalı
- Bilim Dalı: Protetik Diş Tedavisi Bilim Dalı
- Sayfa Sayısı: Belirtilmemiş.
Özet
Amaç: Standart ve frezeli yüzey özelliklerine sahip Grade 4 ve Grade 5 titanyum (Ti), beş farklı dental siman ile olan etkileşimini iki farklı zaman diliminde korozyon riski, bağ dayanımı ve iyon salınımı açısından değerlendirilmesidir. Yöntem: Grade 4 ve 5 Ti disklerden, fabrikasyon ve frezelenmiş yüzeyleri taklit edecek şekilde 6 mm çapında ve 6 mm yüksekliğinde örnekler hazırlandı. Yüzey standardizasyonu sonrasında örnekler üretici talimatları doğrultunda beş farklı dental siman ile simante edildi. Elde dilen Ti sandviçleri, %1 sodyum klorür (NaCl) çözeltisinde 37°C'de 1 ay (t1) ve 3 ay (t2) süreyle inkübe edildi. Mekanik performans makaslama bağ dayanım testiyle, korozyon riski ICP-OES ve IC iyon analizleriyle ve yüzey morfolojisi de taramalı elektron mikroskobu (SEM) ile değerlendirildi. Veriler tek yönlü ANOVA ve bağımsız örneklem t-testi kullanılarak analiz edildi (p<0,05). Bulgular: Siman türü, grade tipi ve inkübasyon süresinin salınan element miktarları üzerinde etkili olduğu belirlendi. Ti iyon salınımı Grade 4 gruplarda siman tipine bağlı olarak tüm dönemlerde anlamlı farklılık gösterdi (p<0,05). Makaslama bağ dayanımı açısından birinci ay sonunda gruplar arasında anlamlı farklılık saptanmazken (p>0,05), üçüncü ay sonunda siman tipine bağlı olarak anlamlı farklar oluştuğu tespit edildi (p<0,05). t2 döneminde Grade 5 gruplarda en yüksek bağ dayanım değerleri polikarboksilat siman, en düşük değerler ise cam iyonomer siman gruplarında izlendi. Tüm gruplarda en sık koheziv başarısızlık izlenirken; polikarboksilat siman uygulanan örneklerde çukurcuk (pitting) korozyonu varlığı saptandı. Sonuç: Polikarboksilat simanların korozyon riskini artırabilmesi nedeniyle özellikle Grade 5 Ti altyapılarda kullanımının dikkatle değerlendirilmesi gerektiği görüldü. Rezin ve cam iyonomer simanların zaman içerisinde bağ dayanımlarında izlenen belirgin azalma ise uzun dönem başarının yalnızca başlangıç retansiyon özelliklerine bağlı olmadığını ortaya koydu. Ti esaslı restorasyonlarda siman seçiminin, biyomateryal bütünlüğünün korunması ve klinik başarının sürdürülebilmesi açısından kritik bir tedavi parametresi olduğu sonucuna varıldı.
Özet (Çeviri)
Objective: To evaluate the effects of five dental cements on the corrosion risk, bond strength, and ion release of Grade 4 and Grade 5 titanium (Ti) with standard and milled surfaces after two incubation periods. Method: Grade 4 and Grade 5 Ti specimens (6 × 6 mm) representing standard and milled implant surfaces were prepared and cemented with five dental cements according to the manufacturers' instructions. The Ti sandwich specimens were incubated in 1% sodium chloride (NaCl) solution at 37°C for 1 month (t1) and 3 months (t2). Shear bond strength was evaluated using a universal testing machine, corrosion by inductively coupled plasma optical emission spectrometry (ICP-OES) and ion chromatography (IC), and surface morphology by scanning electron microscopy (SEM). Data were analyzed using one-way ANOVA and the independent samples t-test (p<0.05). Results: Cement type, titanium grade, and incubation period significantly affected ion release. In Grade 4 groups, Ti ion release differed significantly according to cement type at both time points (p<0.05). Shear bond strength showed no significant differences after 1-month (p>0.05), whereas significant differences were observed after 3-months (p<0.05). At t2, polycarboxylate cement showed the highest bond strength and glass ionomer cement the lowest in Grade 5 groups. Cohesive failure was the predominant failure mode, while pitting corrosion was detected only in the polycarboxylate cement group. Conclusion: Polycarboxylate cement may increase corrosion risk particularly in Grade 5 titanium surfaces and should be used cautiously. The reduction in bond strength over time with resin and glass ionomer cements indicates that long-term performance depends on more than initial retention. Cement selection is critical for titanium restoration longevity.
Benzer Tezler
- Farklı dental implant abutment materyallerine değişik simanların bağlanma dayanımının incelenmesi
Evaluation of the bonding strengths of different cements for different dental implant abutment materials
BURAK KARAMAN
Diş Hekimliği Uzmanlık
Türkçe
2018
Diş HekimliğiGaziosmanpaşa ÜniversitesiProtetik Diş Tedavisi Ana Bilim Dalı
YRD. DOÇ. DR. BİLAL HOLOĞLU
- Dental implant abutmenti - rezin siman bağlantı dayanımı üzerine farklı yüzey pürüzlendirme işlemlerinin etkisinin incelenmesi
Investigation of the Effect of Different Surface Processes on the Bonding Strength of Dental Implant Abutment ? Resin Cement
HASAN GÜNGÖR
Doktora
Türkçe
2010
Diş HekimliğiAtatürk ÜniversitesiProtetik Diş Tedavisi Ana Bilim Dalı
PROF. DR. ZEYNEP YEŞİL DUYMUŞ
- The effect of different surface treatments and bonding agent combinations on the shear bond strength of titanium alloy to lithium disilicate glass-ceramics
Farklı yüzey işlemlerinin ve farklı simanların titanyum tam seramik bağlanma dayanımına etkisi
AFAF EMHAMED MILAD ALKHADASHI
Yüksek Lisans
İngilizce
2017
Diş Hekimliğiİstanbul Yeni Yüzyıl ÜniversitesiProtetik Diş Tedavisi Ana Bilim Dalı
PROF. DR. MELAHAT ÇELİK GÜVEN
- Çeşitli simanlar kullanılarak farklı yükseklik ve genişlikteki abutmentlere simante edilen implant destekli kronların retansiyonlarının in-vitro değerlendirilmesi
Evaluation of the tensile strength of implant supported crown prosthesis luted with various cements to abutments having different heights and widths
EMİNE AYÇA ÇOLAK
Diş Hekimliği Uzmanlık
Türkçe
2019
Diş HekimliğiGazi ÜniversitesiProtetik Diş Tedavisi Ana Bilim Dalı
DOÇ. DR. NEŞET VOLKAN ASAR
- Seramik ve seramik benzeri materyallerin titanyumla adezyonunda rezin simanın ve yüzey işlemlerinin etkisinin incelenmesi
The effect of surface treatments and resin cement on the adhesion of ceramic and ceramic-like materials to titanium
BERKCAN TUNCER
Doktora
Türkçe
2017
Diş HekimliğiHacettepe ÜniversitesiProtez Ana Bilim Dalı
PROF. DR. MEHMET MUHTAROĞULLARI