Farklı ışık kaynakları ile polimerize edilen farklı kompozit rezin restoratif materyallerin monomer değişim derecelerinin mikrosertlik ölçümü ile değerlendirilmesi
Evaluation of degree of conversion of various composite resin restorative materials polymerized by various light sources using microhardness measurement
- Tez No: 260790
- Danışmanlar: DOÇ. DR. MİNE BETÜL ÜÇTAŞLI
- Tez Türü: Doktora
- Konular: Diş Hekimliği, Dentistry
- Anahtar Kelimeler: Kompozit reçineler, Mikrosertlik, Polimerleşme, Composite resins, Microhardness, Polymerization
- Yıl: 2009
- Dil: Türkçe
- Üniversite: Gazi Üniversitesi
- Enstitü: Sağlık Bilimleri Enstitüsü
- Ana Bilim Dalı: Diş Hastalıkları ve Tedavisi Ana Bilim Dalı
- Bilim Dalı: Belirtilmemiş.
- Sayfa Sayısı: Belirtilmemiş.
Özet
Bu çalışmanın amacı, iki farklı ışık cihazı ile üç farklı mesafe ve iki farklı ışık uygulama süresi kullanımı ile polimerize edilen iki farklı kompozit rezinin monomer değişim derecelerinin mikrosertlik ölçümü ile değerlendirilmesidir.Çalışmada 120 adet çekilmiş insan alt 3. büyük azı dişi kullanıldı. Dişlere 3 mm derinlikte standart Sınıf I kaviteler açıldı. Kavite duvarlarına kendinden pürüzlendiren bağlayıcı sistem uygulandı. A2 renginde, biri estetik diğeri akıcı, iki farklı kompozit rezin; tek kütle uygulama tekniği ile kavitelere yerleştirildi. Materyallerin polimerizasyon işlemleri, QTH ve LED ışık cihazları ile gerçekleştirildi. Işık cihazları, 20 sn ve 40 sn, iki farklı sürede ve ışık cihazının ucunun dişlerin tüberkül tepesine olan uzaklığı 0 cm, 0.5 cm ve 1 cm olmak üzere 3 farklı mesafede kullanıldı. Hazırlanan örnekler sert doku kesme cihazı yardımıyla bukko lingual yönde ikiye ayrıldı. Elde edilen örneklerin mikrosertlik ölçümleri, mikrosertlik ölçüm cihazı (HMV-II, Shimadzu, Japonya) kullanılarak 0 mm yüzeyden başlanarak 2.5 mm derinliğe kadar, 6 farklı derinlikte her derinlikte 3 ölçüm yapılarak gerçekleştirildi. Elde edilen değerler istatistiksel analizi yapılmak üzere kaydedildi.İstatistiksel analiz tek yönlü varyans analizi (ANOVA) ve Tamhane testleri ile %95 güven aralığında değerlendirildi.Bu çalışmanın sonucunda, tüm test gruplarında, hibrit kompozit rezin akıcı kompozit rezinden daha yüksek sertlik değerleri gösterdi. Işık uygulama süresinin 20 sn'den 40 sn'ye arttırılması (her iki ışık cihazı için), yüzey sertlik ve monomer değişim derecesi değerlerinde artma sağladı. Işık ucu ile test örneği yüzeyi arasındaki mesafesinin artması, yüzey sertlik ve monomer değişim derecesi değerlerinde azalmaya neden oldu. LED ışık cihazı, QTH ışık cihazlarına oranla daha yüksek yüzey sertlik değerleri ve monomer değişim derecesi gösterdi.
Özet (Çeviri)
The purpose of this study was to evaluate degree of conversion of two different composite resin restorative materials polymerized by using two different light curing units with three different distance and two different light application durations.In this study, 120 extracted human lower third molar teeth were used. Standard class I cavities were prepared and self-etching bonding system was applied to cavities. Two different composite resin restorative materials with A2 color were placed to cavities by bulk technique. Restorative materials were polymerized by using two different light curing units. Light curing units were used on two different irradiation time such as 20 sec and 40 sec with three different distances, 0 cm, 0.5 cm and 1 cm. After restorations, the teeth were divided into two parts by using hard tissue cutting device. Micro hardness measurements were conducted by using micro hardness device (HMV-II, Shimadzu, Japan).Statistical analyses of obtained data were evaluated by ANOVA and Tamhane tests.Following results were observed: for all tested groups, flowable composite showed higher microhardness values then hybrid composite resin. Increase of light use period for light curing units used on the polymerization of composite resin restorative materials provided an increase for microhardness values and monomer conversion degree of material. The increase of distance between light curing units and material surface caused a decrease on the surface microhardness values and monomer conversion degree. LED light curing unit indicated higher microhardness values and monomer conversion degree compared with the QTH light curing unit.
Benzer Tezler
- Lityum disilikat esaslı press-seramik sistemlerinin farklı seramik kalınlıkları ve farklı polimerizasyon yöntemleri kullanıldığında dentine bağlantı etkisinin incelenmesi
Influence of ceramic thickness and polymerization technique on bond strength of a resin luting agent with a lithium disilicate-based press-ceramic system
AKGÜNGÖR NEVAL
- Farklı renk ve kalınlıklardaki zirkonyum seramiklerin ışık geçirgenliği
Light transmission of zirconium ceramics with different color and thickness
İBRAHİM DURAN
- Siloran bazlı bir kompozitin mıkrosızıntı, yüzey sertliği ve düzgünlüğü üzerinde farklı ışık cihazlarının etkileri
Effect of different curing units on microleakage, surface hardness and surface roughness of a silorane based composite
GÖZDE PİRKOCA
- Farklı ışık kaynakları ve ışık uygulama tekniklerinin kompozitlerin mikrosertlik değerleri üzerine etkisi
Effects of different light sources and light curing techniques on microhardness values of composite resins
PINAR KARAKOÇ
- Led ve halojen ışık cihazlarıyla polimerize edilen dört farklı restoratif materyalin sem ile mikrosızıntı açısından incelenmesi
An examination with sem of microleakage of four different restorative materials polymerized with led and halogen light devices
AYŞE GÜNAY