AA 2014 matrisli-B4C parçacık takviyeli kompozit üretimi ve özelliklerinin incelenmesi
Manufacturing of AA 2014 Matrix-B4C particulate composites and investigating properties
- Tez No: 78166
- Danışmanlar: PROF. DR. FAZLI ARSLAN
- Tez Türü: Yüksek Lisans
- Konular: Makine Mühendisliği, Mechanical Engineering
- Anahtar Kelimeler: Bor karbür, Kompozit malzemeler, Mekanik özellikler, Vorteks, Metal matrixcomposites, Particulate composites, Boron carbide, Vortex method, Mechanical properties, Composite materials, Vortex
- Yıl: 1998
- Dil: Türkçe
- Üniversite: Karadeniz Teknik Üniversitesi
- Enstitü: Fen Bilimleri Enstitüsü
- Ana Bilim Dalı: Makine Mühendisliği Ana Bilim Dalı
- Bilim Dalı: Belirtilmemiş.
- Sayfa Sayısı: Belirtilmemiş.
Özet
ÖZET Bu çalışmada matris malzemesi olarak AA 2014 alüminyum alaşımı, parçacık olarak da bor karbür (B4C) kullanılarak sıvı ortamda
Özet (Çeviri)
SUMMARY In this study metal matrix particulate reinforced composite was manufactured using AA2014 alumium alloy matrix and B4C particulate. Mechanical properties of manufactured composites such as hardness, tensile strength and elongation after fracture at different particul volume ratios were also investigated. It is very difficult to manufacture these composites because of bad wetting of liquid matrix of B4C particles. It is necessary to heat the liquid matris up to 1000°C in order to improve wetting properties. But this comparatively high temperature causes Excessive oxidation and gas entrapment in liquid metal. A new method was developped in this study which is based on cleaning of particule surfaces using an acid (% 50 HF +% 50 H2SO4) mixture before mixing with liquit alloy. B4C particles were dried at 150 °C for 12 -24 hours and preheated to 400 °C before adding to liquit alloy at 680°C. The results of microscopic examinations showed the particles were held inthe matrix and homogeneous mixture was obtained. Particle volume ratios were changed between % 1.5 to % 12 and the relations between particle volume ratios hardness and tensile strength and elongation after fracture were investigated. The test results showed that tensile strengths and elongations were decreasing with increasing particle content. This was attributed to ease of crack formation B4C/matris interfaces. Hardness test results indicated that hardness was increasing with particle volume ratio up to % 9. But it was decreasing again because of excessive porosity formation.
Benzer Tezler
- Ovulasyon indüksiyonu tedavisinde folliküler gelişimin ultrasonografik takibi
Başlık çevirisi yok
MERİH BAYRAM
- Bazı esterlerin kinetik incelenmesi ve termodinamik parametrelerin belirlenmesi
Kinetic study and detesmination of thermodnamic parameters of some esters
İBRAHİM TAŞ
- İzmir'de bazı yolların kapatılarak yaya bölgeleri oluşturma da kent peyzajını geliştirme açısından yeniden planlanması üzerinde araştırmalar
Başlık çevirisi yok
BAHAR TÜRKYILMAZ
- Atherosklerotik kalp hastalıklarında risk faktörleri
Risk factors in the coronary artery disease
MURAT SUHER