Geri Dön

Zirkonyanın farklı yüzey işlemleri sonrası rezin siman ile bağlantısının değerlendirilmesi

Effects of surface treatments on the shear bond strenght of luting cements to zirconia

  1. Tez No: 408237
  2. Yazar: IŞIL KEÇİK BÜYÜKHATİPOĞLU
  3. Danışmanlar: DOÇ. DR. ASLI SEÇİLMİŞ, PROF. DR. GÜLFEM ERGÜN
  4. Tez Türü: Doktora
  5. Konular: Diş Hekimliği, Dentistry
  6. Anahtar Kelimeler: Dental bonding, Dental materyaller, Dental restorasyon, Dental stres analizi, Dental çimentolar, Yüzey özellikleri, Zirkonyum, Dental bonding, Dental materials, Dental restoration, Dental stress analysis, Dental cements, Surface properties, Zirconium
  7. Yıl: 2015
  8. Dil: Türkçe
  9. Üniversite: Gaziantep Üniversitesi
  10. Enstitü: Sağlık Bilimleri Enstitüsü
  11. Ana Bilim Dalı: Protetik Diş Tedavisi Ana Bilim Dalı
  12. Bilim Dalı: Belirtilmemiş.
  13. Sayfa Sayısı: Belirtilmemiş.

Özet

Rezin siman ve zirkonya restorasyonlar arasında stabil bağlantıyı sağlamak için uygun simantasyon protokolü halen araştırılan bir konudur. Bu in-vitro çalışmanın amacı, zirkonyaya rezin simanların makaslama bağlantı dayanıklılığına yüzey işlemlerinin etkisini değerlendirmektir. Sinterize zirkonya örnekler (n=192) farklı yüzey işlemi gruplarına ayrılmıştır: Kontrol, kumlama, glaze ve hidroflorik asit uygulaması ve sıcak asit solüsyonu uygulaması (n=48). Her gruptan 12 örnek rastgele seçildi ve yüzey pürüzlülüğü ölçüldü. Daha sonra her bir grup 4 alt gruba ayrıldı (n=12), 3 farklı rezin siman zirkonya yüzeylerine uygulandı. Her bir örneğin makaslama bağlantı dayanımı 5000 termal yaşlandırma sonrası değerlendirildi ve zirkonya örnekler başarısızlık tipinin belirlenmesi için stereomikroskop ile incelendi. Taramalı elektron mikroskop analizi için 2 örnek hazırlandı. Makaslama bağlantı dayanımı değerleri iki yönlü varyans analizi ve Tukey LSD testleri ile analiz edildi. Tek yönlü varyans analizi ve Tukey LSD testleri yüzey pürüzlülük değerlerinin analizi için kullanıldı. Tüm rezin simanlar için, kumlama yüzey işlemi makaslama bağlantı dayanımını arttırdı (p<0.05). Glaze ve hidroflorik asit uygulaması D-SRXU grubu hariç tüm gruplarda makaslama bağlantı dayanımı değerlerini arttırdı (p<0.05). Kumlanmış örneklerin yüzey pürüzlülüğü değerleri kontrol ve deneysel sıcak asit solüsyonu örnekleri ile benzerdi (p>0.05). Glaze grubu en yüksek yüzey pürüzlülüğü değerini sergilemesine rağmen, bu yüzey işlemi tüm gruplar için yüksek makaslama bağlantı dayanımı değeri sağlamadı (p<0.05). Taramalı elektron mikroskobu görüntüleri, makaslama bağlantı dayanımı verilerini destekledi. Bu çalışmanın sonucunda, stabil zirkonya-rezin bağlantısı sağlamak için uygun adheziv/silan bağlayıcı ajan ve yüzey işlemi kombinasyonunun kullanılması önerilebilir.

Özet (Çeviri)

Appropriate cementation protocole is still investigated subject for managing stable bond between resin cement and zirconia restorations. The aim of this in-vitro study was to evaluate the effect of surface treatments on the shear bond strength of resin cements to zirconia. Sintered zirconia specimens (n=192) were divided into different surface treatment groups: Control, sandblasting, glaze and hydrofluoric acid application and hot acid etching application (n=48). Twelve specimens were randomly selected from each group and measured for surface roughness. Then each groups were divided into 4 subgroups (n=12), the 3 different resin cements were adhered onto the zirconia surfaces. Shear bond strenght of each sample was evaluated after 5000 thermal cycles and the zirconia specimens were examined with a stereomicroscope to assess the failure types. two specimens for the scanning electron microscope analysis were prepared. Shear bond strenght values were analyzed through two-way analysis of variance and Tukey LSD tests. One-way analysis of variance and Tukey LSD tests were used for analysis of the surface roughness values. For the all resin cements, the sandblasting surface treatment increased the shear bond strength (p<0.05). The glaze and hydrofluoric acid application increased the shear bond strenght values, except the D-SRXU group (p<0.05). The surface roughness values of the sandblasted specimens were similar with the control and hot etching solution specimens (p>0.05). Although the glaze and hydrofluoric acid group served the highest surface roughness value, this surface treatment was not achieved high shear bond strenght values for all groups (p<0.05). The data of shear bond strenght were supported by the scanning electrone microscopic images. As a result of this study, it can be recommended to use the appropriate combination of the adhesive/silane coupling agent and surface treatment for achieving durable zirconia-resin bonding.

Benzer Tezler

  1. Sinterleme öncesi ve sonrası farklı basınçlarda cam boncuk uygulamasının zirkonya ile rezin simanlar arasındaki bağlantıya etkisinin değerlendirilmesi

    Evaluation the effect of glass-bead air-abrasion at different pressures before and after sintering on the bonding between zirconia and resin cements

    BÜŞRA POLAT

    Diş Hekimliği Uzmanlık

    Türkçe

    Türkçe

    2026

    Diş HekimliğiSağlık Bilimleri Üniversitesi

    Protetik Diş Tedavisi Ana Bilim Dalı

    DR. ÖĞR. ÜYESİ BAHADIR EZMEK

  2. İç yüzey kaplamanın zirkonya restorasyonların bağlanma dayanımına etkisinin in- vitro olarak değerlendirilmesi

    In vitro evaluation of the effect of internal surface coating on the bonding of zirconia restorations

    KUBİLAY ŞENGÜL

    Diş Hekimliği Uzmanlık

    Türkçe

    Türkçe

    2026

    Diş HekimliğiMarmara Üniversitesi

    Protetik Diş Tedavisi Ana Bilim Dalı

    PROF. DR. RİFAT GÖZNELİ

  3. Farklı yüzey işlemlerinin yeni nesil zirkonyanın makaslama bağlantı dayanımına etkisi

    The effect of different surface treatments on the shear bond strength of new generation zirconia

    MERVE BUSE KULTAŞ KALELİ

    Diş Hekimliği Uzmanlık

    Türkçe

    Türkçe

    2022

    Diş HekimliğiSelçuk Üniversitesi

    Protetik Diş Tedavisi Ana Bilim Dalı

    PROF. DR. OĞUZ ERASLAN

  4. Hızlı ve klasik sinterleme uygulanan zirkonyanın farklı yüzey işlemleri sonrası seramik bağlantısının ve mekanik özelliklerinin değerlendirilmesi

    Evaluation of mechanical properties and effects of different surface applications on shear bond strength of porcelain to zirconium oxide after fast and conventional sintering

    MEHMET FEHİM ÇELENK

    Diş Hekimliği Uzmanlık

    Türkçe

    Türkçe

    2016

    Diş HekimliğiCumhuriyet Üniversitesi

    Protetik Diş Tedavisi Ana Bilim Dalı

    YRD. DOÇ. DR. MEHMET EMRE COŞKUN

  5. Zirkonya materyallerinin farklı yüzey bitirme işlemleri sonrası renk değişiminin karşılaştırılması

    Comparison of color change of zirconia materials after different surface finishing processes

    SERAP FALCI

    Doktora

    Türkçe

    Türkçe

    2025

    Diş HekimliğiBaşkent Üniversitesi

    Protetik Diş Tedavisi Ana Bilim Dalı

    PROF. DR. SELİM ERKUT